Influence of Anodization Time and Voltage on the Parameters of TiO2Nanotubes
Open Access
- 1 February 2016
- conference paper
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 116 (1) , 012025
Abstract
A vertically aligned titania nanotube layer was obtained by electrochemical anodic oxidation in the electrolyte contained 0.4 wt% solution of NH 4 F in 54 ml of ethylene glycol and 5 ml of deionized water, after titanium was chemically cleaned/etched with a mixture of HCl, H 2 O and HNO 3 solution for removing the natural oxide films. The morphology and composition of the titania nanotube layer were examined by scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). The anodization of TiO 2 nanotubes was done using 60 V for 240 min and 30 min, and 30 V for 30 min. The diameter of the titania nanotubes was about 52-156 nm, the wall thickness about 32-53 nm and the height about 0.9-6.3 μm. The pore size of TiO 2 nanotubes influences the dissolution rate of CaP thin films and Young's modulus, which is significantly lower than that of the Ti substrate. Our future challenge will be investigation of the microstructure and mechanical behavior of titania nanotubes with CaP film.Keywords
This publication has 5 references indexed in Scilit:
- Titania nanotube porosity controls dissolution rate of sputter deposited calcium phosphate (CaP) thin film coatingsRSC Advances, 2013
- Hydroxyapatite coating on titanium surface with titania nanotube layer and its bond strength to substrateJournal of Porous Materials, 2009
- Microstructure and deformation behavior of biocompatible TiO2 nanotubes on titanium substrate☆Acta Biomaterialia, 2007
- Growth of nano-scale hydroxyapatite using chemically treated titanium oxide nanotubesBiomaterials, 2005
- High‐Aspect‐Ratio TiO2 Nanotubes by Anodization of TitaniumAngewandte Chemie International Edition, 2005