Reduction of Sr2MnO4 Investigated by High Temperature in Situ Neutron Powder Diffraction under Hydrogen Flow
- 7 January 2013
- journal article
- research article
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 52 (2) , 1009-1017
Abstract
This experiment emphasizes the first example of two-phase sequential Rietveld refinements throughout a solid/gas chemical reaction monitored by Neutron Powder Diffraction (NPD) at high temperature. The reduction of the n = 1 Ruddlesden–Popper (RP) oxide Sr2MnO4 heated under a flow of 5% H2–He has been investigated throughout two heating/cooling cycles involving isothermal heating at 500 and 550 °C. Oxygen loss proceeds above T ∼ 470 °C and increases with temperature and time. When the oxygen deintercalated from the “MnO2” equatorial layers of the structure results in the Sr2MnO3.69(2) composition, the RP phase undergoes a first order I4/mmm → P21/c, tetragonal to monoclinic phase transition as observed from time-resolved in situ NPD. The phase transition proceeds at 500 °C but is incomplete; the weight ratio of the P21/c phase reaches ∼41% after 130 min of isothermal heating. The fraction of the monoclinic phase increases with increasing temperature and the phase transition is complete after 80 min of isothermal heating at 550 °C. The composition of the reduced material refined to Sr2MnO3.55(1) and does not vary on extended heating at 550 °C and subsequent cooling to room temperature (RT). The symmetry of Sr2MnO3.55(1) is monoclinic at 550 °C and therefore consistent with the RT structure determined previously for the Sr2MnO3.64 composition obtained from ex situ reduction. Consequently, the stresses due to phase changes on heating/cooling in reducing atmosphere may be minimized. The rate constants for the reduction of Sr2MnO4.00 determined from the evolution of weight ratio of the tetragonal and monoclinic phase in the time-resolved isothermal NPD data collected on the isotherms at 500 and 550 °C are k500 = 0.110 × 10–2 and k550 = 0.516 × 10–2 min–1 giving an activation energy of ∼163 kJ mol–1 for the oxygen deintercalation reaction.Keywords
This publication has 36 references indexed in Scilit:
- Physicochemical properties of non-stoichiometric oxidesJournal of Thermal Analysis and Calorimetry, 2010
- Recent developments in Ruddlesden–Popper nickelate systems for solid oxide fuel cell cathodesJournal of Solid State Electrochemistry, 2006
- Anisotropic ionic transport properties in La2NiO4+δ single crystalsSolid State Ionics, 2004
- Chemical oxygen diffusion coefficient measurement by conductivity relaxation—correlation between tracer diffusion coefficient and chemical diffusion coefficientJournal of the European Ceramic Society, 2004
- Mass transport in La2Ni1−xCoxO4+δ oxides with the K2NiF4 structureSolid State Ionics, 2002
- Oxygen diffusion and surface exchange in La2−xSrxNiO4+δSolid State Ionics, 2000
- A comparison of the transport properties of La2−xSrxNi1−yFeyO4+δ where 0<x<0.2 and 0<y<0.2Ionics, 1999
- Crystal and magnetic structures of the colossal magnetoresistance manganates (x=0.0, 0.1)Physical Review B, 1996
- Giant magnetoresistance of manganese oxides with a layered perovskite structureNature, 1996
- Ceramic Fuel CellsJournal of the American Ceramic Society, 1993