Mechanism of crack path morphology and branching from small fatigue cracks under mixed loading
- 9 September 2004
- journal article
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 28 (1-2) , 49-60
Abstract
In order to investigate the crack path in materials containing a small crack under mixed mode loading, reversed torsion and combined push–pull/torsion fatigue tests were carried out on 0.47% carbon steel specimens containing an initial small crack. The initial small cracks were introduced by a preliminary push–pull fatigue test using a specimen that contained an artificial small hole of 40 μm diameter/depth. Push–pull fatigue tests followed by reversed torsion, and reversed torsion followed by push–pull were carried out. Fatigue tests of combined push–pull/torsion followed by push–pull were also carried out to examine the effect of crack geometry, such as branching and kinking, on cumulative fatigue damage. Different crack growth behaviours due to different loading modes and sequences complicatedly influenced the fatigue crack path and eventually the cumulative fatigue damage. Thus, existing fatigue damage theories cannot be applied to the cases presented in this study. A single factory roof morphology was formed on the fracture surface of the specimen having an initial semielliptical surface crack under cyclic torsion. Taking the result into consideration, torsional fatigue tests of circumferentially cracked specimens were carried out to investigate the Mode III crack growth threshold and the formation mechanism of the factory roof. It was found that the factory‐roof pattern was formed by Mode I crack branching from small semielliptical cracks nucleated ahead of the circumferential crack tip. Thus, stress intensity factors at the semielliptical crack tip ahead of the circumferential crack tip were analysed to make the mechanism of crack branching from the semielliptical crack clear. The analysis shows that the Mode III stress intensity factor, KIII, at the deepest point of the semielliptical crack decreases with increase in the depth of semielliptical crack. It follows that as the shear crack growth becomes difficult at the semielliptical crack tip, crack branching starts at the major axis ends in the direction for Mode I growth, forming factory roof, due to ΔKIth < ΔKIIIth.Keywords
This publication has 16 references indexed in Scilit:
- Threshold and growth mechanism of fatigue cracks under mode II and III loadingsFatigue & Fracture of Engineering Materials & Structures, 2003
- Multiaxial Fatigue1999
- TORSIONAL FATIGUE OF A MEDIUM CARBON STEEL CONTAINING AN INITIAL SMALL SURFACE CRACK INTRODUCED BY TENSION–COMPRESSION FATIGUE: CRACK BRANCHING, NON‐PROPAGATION AND FATIGUE LIMITFatigue & Fracture of Engineering Materials & Structures, 1998
- A STUDY OF CUMULATIVE FATIGUE DAMAGE UNDER VARIABLE LOADING‐MODE CONDITIONSFatigue & Fracture of Engineering Materials & Structures, 1996
- Fatigue and Creep-Fatigue Damage of Austenitic Stainless Steels under Multiaxial LoadingMetallurgical Transactions A, 1993
- Effect of load sequence on fatigue damage accumulation of a low carbon steel under rotating bending and cyclic torsion.TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A, 1987
- Mode III fatigue crack propagation in low alloy steelMetallurgical Transactions A, 1982
- The quarter-infinite crack in a half space; Alternative and additional solutionsInternational Journal of Solids and Structures, 1980
- The mode III fatigue crack growth threshold for mild steelInternational Journal of Fracture, 1979
- State of stress at the vertex of a quarter-infinite crack in a half-spaceInternational Journal of Solids and Structures, 1977