Origin of High Coercivity in Chemically Deposited Cobalt-Phosphorus Films
Authors:
- 1 March 1966
- journal article
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 37 (3) , 1158-1159
Abstract
Films of Co-P, varying in composition from 2.5% to 5% P and varying in thickness from 200 to 2500 Å, were prepared by chemical deposition. The coercivity of these films was found to be a function of both P content and thickness. The particle size of these films increased with increasing thickness and was a function of the P content. The films were annealed in a reducing atmosphere at various temperatures up to 500°C. The low-coercivity films undergo a transformation to films exhibiting coercivities of ∼250 Oe at a temperature of 250°C. The intermediate-coercivity films remain essentially unchanged, whereas the high-coercivity films drop sharply in coercivity at ∼400°C to this apparent ``equilibrium coercivity'' of ∼250 Oe. Etching experiments on these samples show no drastic effects on coercivity. The coercivity merely proceeds back along the original coercivity-versus-thickness curves. Structural and magnetic evidence indicates the existence of an equilibrium magnetic structure in these films which is primarily dependent on particle size.Keywords
This publication has 3 references indexed in Scilit:
- Magnetic Properties and Corrosion Behavior of Thin Electroless Co-P DepositsJournal of the Electrochemical Society, 1965
- Magnetic Films of Electroless Cobalt -Phosphorus with Uniaxial AnisotropyJournal of the Electrochemical Society, 1964
- Preparation and Magnetic Characteristics of Chemically Deposited Cobalt for High-Density StorageJournal of the Electrochemical Society, 1962