Thermal Expansion Characteristics of Alumina–Magnesia and Alumina–Spinel Castables in the Temperature Range 800°–1650°C
Authors:
- 1 November 2000
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 83 (11) , 2872-2874
Abstract
The thermal expansion of Al2O3–MgO castables containing 5.5 wt% MgO and 1.36 wt% CaO and Al2O3–spinel castables containing 20 wt% spinel having 95 wt% Al2O3 and 1.7 wt% CaO was measured in the temperature range of 800–1650°C by dilatometry. A sharp increase in expansion from around 1425° to 1525°C, followed by a sharp decrease with further increasing temperature, is characteristic of Al2O3–MgO castables. The sharp increase in expansion is believed to be caused by the bond linkage between the CA6 and spinel grains in the bonding matrix, while the sharp decrease is apparently related to liquid‐phase sintering. The sharp increase and decrease in expansion were not observed in Al2O3–spinel castables because of the much lower MgO (around 1 wt% MgO) and impurity contents. The magnitude of thermal expansion of calcium aluminate bonded castables containing self‐forming or preforming spinels or both is dictated by the MgO content of the castables.Keywords
This publication has 2 references indexed in Scilit:
- Effect of spinel content on hot strength of alumina-spinel castables in the temperature range 1000–1500°CJournal of the European Ceramic Society, 1999
- Effect of CaO Content on the Hot Strength of Alumina‐Spinel Castables in the Temperature Range of 1000° to 1500°CJournal of the American Ceramic Society, 1998