We demonstrated high-performance 8.9 μm cutoff wavelength nBn InAs/InAsSb type-II strained-layer superlattice (T2SL). These detectors exhibit a long minority carrier (hole) lifetime of 1.2 μs at 80 K, high quantum efficiency of 40% for back-side illuminated devices without antireflection coating, and low dark current density of 4.6 × 10−6 A/cm2 at 80 K. We measured absorption, minority carrier (hole) lifetime, quantum efficiency, and spectral response as a function of the temperature and applied bias. We investigated the temperature dependence of the hole diffusion length and mobility and found that their values increase with temperature from 1.3 μm and 6.5 cm2/Vs at 30 K to 6.5 μm and 36 cm2/Vs at T = 90 K. We compared the measured diffusion length and mobility of holes in long-wavelength infrared (LWIR) T2SL with these parameters of a high-performance mid-wavelength infrared (MWIR) T2SL. Unexpectedly, hole mobility in LWIR T2SL was found to be higher than in MWIR that is contrary to the theoretical predictions.Keywords
Funding Information
- Earth Sciences Division
- U.S. Department of War
This publication has 25 references indexed in Scilit:
- Long Wavelength InAs/InAsSb Infrared Superlattice Challenges: A Theoretical InvestigationJournal of Electronic Materials, 2020
- Carrier Transport in the Valence Band of nBn III–V Superlattice Infrared DetectorsJournal of Electronic Materials, 2019
- Dark current reduction in microjunction-based double electron barrier type-II InAs/InAsSb superlattice long-wavelength infrared photodetectorsScientific Reports, 2017
- Type-II superlattice hole effective massesInfrared Physics & Technology, 2017
- Theoretical Aspects of Minority Carrier Extraction in Unipolar Barrier Infrared DetectorsJournal of Electronic Materials, 2015
- Significantly improved minority carrier lifetime observed in a long-wavelength infrared III-V type-II superlattice comprised of InAs/InAsSbApplied Physics Letters, 2011
- Type-II Superlattice Infrared Detectors2011
- Carrier lifetime measurements in short-period InAs/GaSb strained-layer superlattice structuresApplied Physics Letters, 2009
- n B n detector, an infrared detector with reduced dark current and higher operating temperatureApplied Physics Letters, 2006
- Back side reflection influence on quantum efficiency of photovoltaic devicesElectronics Letters, 1988