The effects of devulcanize microwave radiation time on crosslink density of EPDM waste/natural rubber blend
Authors:
- Nurul Adilah Shahrul FaizalNFNurul Adilah Shahrul Faizal
- Dalina SamsudinDSDalina Samsudin
- Norhidayah Ahmad JaliniNJNorhidayah Ahmad Jalini
- Zuliahani AhmadZAZuliahani Ahmad
- Muhamad Naiman SaripMSMuhamad Naiman Sarip
- Nor Mazlina Abdul WahabNWNor Mazlina Abdul Wahab
- Mohd Syamaizar MustafaMMMohd Syamaizar Mustafa
- 26 February 2021
- conference paper
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2332 (1) , 100003
Abstract
Ethylene Propylene Diene Monomer Rubber (EPDM) waste is a vulcanize rubber waste that content a highly crosslinking molecular structure which makes recycling and waste management of the EPDM waste to be a challenge. Hence, the microwave devulcanization method is one of the most promising method to recycle rubber waste as it gives a uniform heating throughout the rubber waste. The microwave radiation may effectively break the rubber waste crosslink molecular structure. In this study, grind EPDM (G-EPDM) was devulcanize at a different exposure microwave radiation time (3, 5, 7 and 9 minutes) and blended with natural rubber (NR). Then, the blends were characterized for Fourier Transform Infrared (FTIR), cure characteristics, swelling, and crosslink density. The Fourier Transform Infrared (FTIR) spectrum of the microwave devulcanized EPDM shows changes after the radiation. The FTIR spectrum of G-EPDM and microwave devulcanized EPDM was focused at wavenumber of 1659 cm−1 (C=C link), 1532 cm−1 (methyl-assisted conjugated double bond), 1392 cm−1 (CH3) and 856 cm-1 (RC=CH2 group). Observed of spectrum changes after the G- EPDM was exposed to the microwave radiation. Meanwhile, the infrared spectrum of NR/G-EPDM and NR/M (5)–EPDM, were studied at wavenumber of 1272 cm-1, 962.3 cm−1, and 874 cm−1 and 667 cm−1 indicate the C-N aromatic group, S-O bond and C-S bond, respectively. From G-EPDM until 5 minutes exposure times, crosslink density shows an increment pattern of 21.13% conversely swelling of rubber which shows a decrement pattern of 5.14 %.Keywords
This publication has 12 references indexed in Scilit:
- Cure and Degradation Kinetics of Sulfur Cured Nanocomposites of EPDM-NBR Rubber BlendsMaterials Today: Proceedings, 2018
- Recycling of rubber wastes by devulcanizationResources, Conservation and Recycling, 2018
- Devulcanization of waste tire rubber by microwavesPolymer Degradation and Stability, 2017
- The effect of the addition of alkanolamide on properties of carbon black-filled natural rubber (SMR-L) compounds cured using various curing systemsPolymer Testing, 2016
- Devulcanization of ground tire rubber: Physical and chemical changes after different microwave exposure timesExpress Polymer Letters, 2015
- A novel industrial technique for recycling ethylene-propylene-diene waste rubberPolymer Degradation and Stability, 2015
- Effects of virgin Ethylene–Propylene–Diene–Monomer and its preheating time on the properties of natural rubber/recycled Ethylene–Propylene–Diene–Monomer blendsMaterials & Design (1980-2015), 2013
- Comparison of thermo-oxidative ageing and thermal analysis of carbon black-filled NR/Virgin EPDM and NR/Recycled EPDM blendsPolymer Testing, 2013
- Use of styrene butadiene rubber industrial waste devulcanized by microwave in rubber composites for automotive applicationMaterials & Design (1980-2015), 2012
- Dynamic mechanical properties and swelling behaviour of NR/reclaimed rubber blendsMaterials Letters, 2003