Changes in the Structure of a Thermal Protective Nickel Aluminide Coating under the Influence of a Single Thermal Laser Pulse
- 30 May 2022
- journal article
- research article
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (3) , 740-744
Abstract
The regularities of changes in the structure and phase composition of a thermal protective nickel aluminide coating (45% Ni, 14% Al, 22% Co, 18.9% Cr, 0.15% Fe, 0.14% Nb, 0.09% Y, 0.06% Ca, 0.01% Mn, 0.15% C, 0.15% Si, and 0.006% S) after exposure to short-term pulsed heat fluxes of various power created by the radiation of an LRS-150A pulse-periodic laser with a radiation wavelength λ = 1.06 μm and a pulse duration τ = 12 × 10–3 s were studied. The radiation energy was E = 5, 10, and 15 J. Microstructural analysis and the elemental composition of the resulting coating were carried out as well as analysis of the phase composition. X-ray microanalysis of the coating was also carried out. In the initial state and after irradiation of the coating with a heat flux power P = 7 × 103 W/cm2, light microregions are observed on the micrographs of the surface. These regions do not have clearly defined external boundaries and consist of the NiAl phase and a small amount of the Ni3Al phase with the presence of inclusions of particles containing a solid solution of Ni–Co–Cr. After irradiation of the coating with heat fluxes of higher power (P = 1.7 × 104 W/cm2 and P = 2.2 × 104 W/cm2), large convex formations appeared on its surface, consisting mainly of Ni3Al and NiAl phases. On micrographs of the surface, they appear as white areas with well-defined outer boundaries. The content of the Ni3Al phase in them increased in comparison with the initial state and the content of the NiAl phase decreased, while the particles of inclusions of Ni, Co, and Cr disappeared. It can be assumed that an increase in the Ni3Al content is associated with the dissolution of particles of a solid solution of Ni–Co and Cr in the melt and the subsequent diffusion of nickel into the NiAl phase. When exposed to a heat flux of power P = 2.2 × 104 W/cm2, microcracks appear on the areas of the coating surface covered with aluminum oxide.Keywords
This publication has 7 references indexed in Scilit:
- Change in the Morphology of the Surface of Ta–W Coating after Exposure to Cyclic Laser PulsesInorganic Materials: Applied Research, 2019
- Investigation of Heat Resistance of Al-Ni Layered CoatingSolid State Phenomena, 2017
- Influence of cyclic laser pulses on degradation of a tantalum coatingInorganic Materials: Applied Research, 2017
- Development and postoperation state of Ni–Co–Cr–Al–Y plasma heat-resistant coatingJournal of Machinery Manufacture and Reliability, 2016
- The structure and physical-mechanical properties of the heat-resistant Ni-Co-Cr-Al-Y intermetallic coating obtained using rebuilt plasma equipmentThermophysics and Aeromechanics, 2014
- Micropyretic synthesis of tough NiAl alloysMetallurgical and Materials Transactions B, 1997
- NiAl alloys for high-temperature structural applicationsJOM, 1991