Static and Dynamic Fibrous Initiation Toughness Results for Nine Pressure Vessel Materials
Author:
- 1 January 1979
- book chapter
- Published by ASTM International
- p. 493-514
Abstract
The upper-shelf toughness regime corresponds to the normal operating temperature for ferritic nuclear pressure vessels. However, actual fibrous initiation toughness data have not been available for a wide variety of heats of steels and weldments. In fact, much of the data available have assumed that fracture initiation occurred at maximum load (equivalent energy approach), which is not the case for most materials tested on the upper shelf. Multispecimen (25.4 mm thickness compact or bend) initiation tests were, therefore, performed in the upper shelf temperature region to determine JIc for five base metal (two A533B-1, one A508-2, and two A302B) and four weld metal (two manual arc and two submerged arc) heats of nuclear ferritic steel. All of the heats were investigated under quasi-static loading (loading time ∼ 100 s) and under either closed-loop hydraulic loading (loading time ∼ 100 ms) or controlled impact loading (loading time ∼ 1 ms). For all materials investigated, crack initiation occurred prior to maximum load, and initiation toughness values (KJc) were up to 50 percent less than the equivalent energy (maximum load) toughness values. The initiation toughness results at 177°C also increased with decreasing loading time for all but one heat tested. HSST Plate 02 (A533B-1 steel) was tested at 71°C using all three loading rates; there were little differences observed for the Plate 02 tests due to loading rate, although the intermediate loading rate results were slightly lower than the rest. The data were analyzed using a simple statistical approach to obtain approximate confidence limits for the JIc values obtained. A comparison of JIc values obtained using three-point and nine-point fibrous crack length averages across the specimen thickness was made. The nine-point average generally gave higher values of JIc, but the variance about the regression line was not consistently lower than for the three-point average.Keywords
This publication has 7 references indexed in Scilit:
- Analysis of radiation embrittlement reference toughness curves. Final report1981
- Structural Integrity of Water Reactor Pressure Boundary Components.1979
- General Yielding of Charpy V-Notch and Precracked Charpy SpecimensJournal of Engineering Materials and Technology, 1978
- Impact Three-Point Bend Testing for Notched and Precracked SpecimensJournal of Testing and Evaluation, 1978
- Recent Developments in JIc Testing1977
- An experimental investigation of the effect of specimen type on the crack tip opening displacement and J-integral fracture criteriaInternational Journal of Fracture, 1976
- A J Integral Analysis for the Compact Specimen, Considering Axial Force as Well as Bending EffectsJournal of Pressure Vessel Technology, 1974