Heat Induced Structure Modifications in Polymer‐Layered Silicate Nanocomposites
- 24 August 2004
- journal article
- research article
- Published by Wiley in Macromolecular Materials and Engineering
- Vol. 289 (9) , 783-786
Abstract
Summary: The success of the use of layered silicates in polymer nanocomposites, to improve physical and chemical properties is strictly related to a deeper knowledge of the mechanistic aspects on which the final features are grounded. This work shows the temperature induced structural rearrangements of nanocomposites based on poly[ethylene‐co‐(vinyl acetate)] (EVA) intercalated‐organomodified clay (at 3–30 wt.‐% silicate addition) which occur in the range between 75 and 350 °C. In situ high temperature X‐ray diffraction (HT‐XRD) studies have been performed under both nitrogen and air to monitor the modifications of the nanocomposite structure at increasing temperatures under inert/oxidative atmosphere. Heating between 75 and 225 °C, under nitrogen or air, causes the layered silicate to migrate towards the nanocomposite surface and to increase its interlayer distance. The degradation of both the clay organomodifier and the VA units of the EVA polymer seems to play a key role in driving the evolution of the silicate phase in the low temperature range. The structural modifications of the nanocomposites in the high temperature range (250–350 °C), depended on the atmosphere, either inert or oxidizing, in which the samples were heated. Heating under nitrogen led to deintercalation and thus a decrease of the silicate interlayer space, whereas exfoliation was the main process under air leading to an increase of the silicate interlayer space. Heat induced structural modification of EVA‐clay nanocomposite under nitrogen and air. magnified image Heat induced structural modification of EVA‐clay nanocomposite under nitrogen and air.Keywords
This publication has 9 references indexed in Scilit:
- Processing degradation of polyamide 6/montmorillonite clay nanocomposites and clay organic modifierPolymer Degradation and Stability, 2003
- Some comments on the modes of action of nanocomposites in the flame retardancy of polymersFire and Materials, 2003
- Cone Calorimeter Combustion and Gasification Studies of Polymer Layered Silicate NanocompositesChemistry of Materials, 2002
- Thermal Degradation Chemistry of Alkyl Quaternary Ammonium MontmorilloniteChemistry of Materials, 2001
- Combustion behaviour of EVA/fluorohectorite nanocompositesPolymer Degradation and Stability, 2001
- Polymer-layered silicate nanocomposites: preparation, properties and uses of a new class of materialsMaterials Science and Engineering: R: Reports, 2000
- Aspects of the thermal oxidation of ethylene vinyl acetate copolymerPolymer Degradation and Stability, 2000
- Thermal degradation of vinyl acetate—methacrylic acid copolymer and homopolymers. I. An FTIR spectroscopic investigation of structural changes in the degrading materialPolymer Degradation and Stability, 1995
- Thermal degradation of vinyl acetate-methacrylic acid copolymer and the homopolymers. II. Thermal analysis studiesPolymer Degradation and Stability, 1995