Corrosion failure analysis of a perforated F32 reactor
Authors:
- 28 May 2019
- journal article
- research article
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 61 (6) , 533-536
Abstract
The principle reason for corrosion failure because of perforation on a fluorination reactor was analyzed by chemical composition tests, microstructure and corrosion products observation tests in combination with the investigation of the working conditions of the reactor. The results show that a certain amount of complex inclusions containing MnS in the failure parts – are the principle cause of perforation. The relatively poor condition of the middle of the reactor, resulting in particular from excess hydrogen fluoride, is another principle cause.Keywords
This publication has 5 references indexed in Scilit:
- Effects of concentrated rigid inclusions defects on the in-plane impact behavior of hexagonal honeycombsJournal of Mechanical Science and Technology, 2017
- Electrochemical investigation on the hydrogen permeation behavior of 7075-T6 Al alloy and its influence on stress corrosion crackingInternational Journal of Minerals, Metallurgy and Materials, 2015
- The mechanism of hydrogen-induced pitting corrosion in duplex stainless steel studied by SKPFMCorrosion Science, 2012
- A study on the initiation of pitting corrosion in carbon steel in chloride-containing media using scanning electrochemical probesElectrochimica Acta, 2010
- Effect of H2S on stress corrosion cracking and hydrogen permeation behaviour of X56 grade steel in atmospheric environmentCorrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control, 2009