Structure and magnetism of Fe-dopedSnO2nanoparticles

Authors:

Abstract
SnO2 nanoparticles doped with Fe of different concentrations were synthesized by a chemical coprecipitation method. After calcination at 600 °C, the samples were characterized using x-ray diffraction (XRD), transmission electron microscope (TEM), and superconducting quantum interference device magnetometer. XRD shows that the solubility of Fe in SnO2 (Sn1−xFexO2: primary phase where Fe substitutes Sn in SnO2 matrix) is less than 7.5% (x<0.075) and Fe2O3 (hematite) or (Fe1−ySny)2O3 (where Sn substitutes Fe in Fe2O3 matrix) is evolved as a secondary phase for x≥0.075 along with Sn1−xFexO2 (primary phase). TEM shows that the particles are crystalline and of size in the nanometric regime (10±3 nm). The M(T) and M(H) studies indicated an antiferromagnetic (AFM) interaction in 3% and 5% (atomic weight) Fe-doped SnO2 nanoparticles. The observed AFM interaction can be explained by the bound magnetic polaron model for insulating diluted magnetic semiconductor systems. It is seen that the strength of AFM interaction reduces with increase in doping concentration. On the other hand, 7.5% Fe-doped SnO2 nanoparticles show the ferromagnetic interaction, but the origin of the observed ferromagnetism is identified due to the presence of (Fe1−ySny)2O3 as a secondary phase.

This publication has 58 references indexed in Scilit: