Formation of fine grained structure in a magnesium alloy AZ31 during multi-directional forging with decreasing deformation temperature
Authors:
- Jie XingJXJie Xing
- Hiroshi SodaHSHiroshi Soda
- Xuyue YangXYXuyue Yang
- Hiromi MiuraHMHiromi Miura
- Taku SakaiTSTaku Sakai
Open Access
- 1 January 2004
- journal article
- Published by Japan Institute of Light Metals in Journal of Japan Institute of Light Metals
- Vol. 54 (11) , 527-531
Abstract
No abstract availableKeywords
This publication has 10 references indexed in Scilit:
- Initial Grain Size Effect of Dynamic Recrystallization of Magnesium Alloy AZ31Materials Science Forum, 2003
- Grain-Boundary Sliding in AZ31 Magnesium Alloys at Room Temperature to 523 KMATERIALS TRANSACTIONS, 2003
- Effect of microstructural factors on tensile properties of ECAE-processed AZ31 magnesium alloy.Journal of Japan Institute of Light Metals, 2002
- Dynamic evolution of fine grain structure during hot deformation of an AZ31 magnesium alloy.Journal of Japan Institute of Light Metals, 2002
- Grain refinement in copper under large strain deformationPhilosophical Magazine A, 2001
- MagnesiumMaterials Science and Engineering: A, 2001
- Plastic Deformation: Role of Recovery and Recrystallization2001
- Plastic-forming processes for magnesium alloysJournal of Japan Institute of Light Metals, 2001
- Strain-induced submicrocrystalline grains developed in austenitic stainless steel under severe warm deformationPhilosophical Magazine Letters, 2000
- Effect of True Strain Rate Control on Hot Compression of a 3%Si SteelJournal of the Japan Institute of Metals and Materials, 1991