Abstract
We report the effect of $$\delta${}$ doping at the LaAlO${}_{3}$/SrTiO${}_{3}$ interface with LaMnO${}_{3}$ monolayers on the photoconducting (PC) state. The PC is realized by exposing the samples to broadband optical radiation of a quartz lamp and 325 and 441 nm lines of a He-Cd laser. Along with the significant modification in electrical transport which drives the pure LaAlO${}_{3}$/SrTiO${}_{3}$ interface from metal-to-insulator with increasing LaMnO${}_{3}$ sub-monolayer thickness, we also observe an enhancement in the photoresponse and relaxation time constant. A possible scenario for the PC based on defect clusters, random potential fluctuations, and large lattice relaxation models, along with the role of structural phase transition in SrTiO${}_{3}$, is discussed. For pure LaAlO${}_{3}$/SrTiO${}_{3}$, the photoconductivity appears to originate from interband transitions between Ti-derived $3d$ bands which are ${e}_{g}$ in character and O 2$p$\char21{}Ti ${t}_{2g}$ hybridized bands. The band structure changes significantly when fractional layers of LaMnO${}_{3}$ are introduced. Here the Mn ${e}_{g}$ bands ($$\approx${}$1.5 eV above the Fermi energy) within the photoconducting gap lead to a reduction in the photoexcitation energy and a gain in overall photoconductivity.
All Related Versions