Temporal pulse shaping: a key parameter for the laser welding of dental alloys
- 10 June 2014
- journal article
- Published by Springer Nature in Lasers in Medical Science
- Vol. 30 (5) , 1457-1464
Abstract
This study aims to describe the effect of pulse shaping on the prevention of internal defects during laser welding for two dental alloys mainly used in prosthetic dentistry. Single spot, weld beads, and welds with 80 % overlapping were performed on Co-Cr-Mo and Pd-Ag-Sn cast plates with a pulsed neodymium-doped yttrium aluminum garnet (Nd:YAG) laser. A specific welding procedure using adapted parameters to each alloy was completed. All the possibilities for pulse shaping were tested: (1) the square pulse shape as a default setting, (2) a rising edge slope for gradual heating, (3) a falling edge slope to slow the cooling process, and (4) a combination of rising and falling edges. The optimization of the pulse shape is supposed to produce defect-free welds (crack, pores, voids). Cross-section SEM observations and Vickers microhardness measurements were made. Pd-Ag-Sn was highly sensitive to hot cracking, and Co-Cr-Mo was more sensitive to voids and small porosities (sometimes combined with cracks). Using a slow cooling ramp allowed a better control on the solidification process for those two alloys always preventing internal defects. A rapid slope should be preferred for Co-Cr-Mo alloys due to its low-laser beam reflectivity. On the opposite, for Pd-Ag-Sn alloy, a slow rising slope should be preferred because this alloy has a high-laser beam reflectivity.Keywords
This publication has 26 references indexed in Scilit:
- Effect of the combination of different welding parameters on melting characteristics of grade 1 titanium with a pulsed Nd–Yag laserLasers in Medical Science, 2007
- Effect of grain boundary characteristics on hot tearing in directional solidification of superalloysJournal of Materials Research, 2006
- Nd:YAG laser penetration into cast titanium and gold alloy with different surface preparationsJournal of Oral Rehabilitation, 2006
- Hot cracking in Al–Mg–Si alloy laser welding – operating parameters and their effectsMaterials Science and Engineering: A, 2005
- Optimization of operator and physical parameters for laser welding of dental materialsBritish Dental Journal, 2004
- Keyhole formation and power deposition in Nd:YAG laser spot weldingJournal of Physics D: Applied Physics, 2001
- The laser welding technique applied to the non precious dental alloys procedure and resultsBritish Dental Journal, 2001
- Study of voluminal defects observed in laser spot welding of tantalumJournal of Physics D: Applied Physics, 2000
- Solidification crack susceptibility of laser weld metal in 0.2C‐Ni‐Cr‐Mo steels: Effects of bead configuration and S and P contentsWelding International, 1993
- Cracking in laser welds of dental Ni-Cr alloys. Effect of alloy composition.Nihon Hotetsu Shika Gakkai Zasshi, 1990