Dissolution and erosion behavior of AISI H13 shot sleeve in high pressure die casting process
Authors:
- H. VachhaniHVH. Vachhani
- M. RathodMRM. Rathod
- R. ShahRSR. Shah
- 1 July 2019
- journal article
- research article
- Published by Elsevier in Engineering Failure Analysis
- Vol. 101, 206-214
Abstract
No abstract availableKeywords
Funding Information
- Firodia Scholarship Trust
- JAYA-HIND Industries ltd-Pune
- College of Engineering, Pune,
This publication has 8 references indexed in Scilit:
- Effect of Si Content on Wear Performance of Hot Work Tool SteelTribology Letters, 2016
- Erosion process analysis of die-casting inserts for magnesium alloy componentsEngineering Failure Analysis, 2013
- Sliding wear of CrN, AlCrN and AlTiN coated AISI H13 hot work tool steels in aluminium extrusionTribology International, 2013
- Thermal fatigue properties of differently constructed functionally graded materials aimed for refurbishing of pressure-die-casting diesEngineering Failure Analysis, 2012
- Thermo fatigue cracking of die casting diesEngineering Failure Analysis, 2012
- Effect of surface roughness on the properties of the layer formed on AISI 304 stainless steel after plasma nitridingSurface and Coatings Technology, 2006
- Investigating ion nitriding for the reduction of dissolution and soldering in die-casting shot sleevesSurface and Coatings Technology, 2003
- Effects of molten aluminum on H13 dies and coatingsJournal of Materials Engineering and Performance, 1995