Abstract
Significant increases in the critical fracture toughness (KIC) over that of alumina are obtained by the stress‐induced phase transformation in partially stabilized ZrO2 particles which are dispersed in alumina. More importantly, improved slow crack growth resistance is observed in the alumina ceramics containing partially stabilized ZrO2 particles when the stress‐induced phase transformation occurs. Thus, increasing the contribution of the ZrO2 phase transformation by tailoring the Y2O3 stabilizer content not only increases the critical fracture toughness (KIC) but also the KIa to initiate slow crack growth. For example, crack velocities (v)≥10–9 m/s are obtained only at KIa≥5 MPa.m1/2 in transformation‐toughened (KIC=8.5 MPa.m1/2) composites vs KIa≥2.7 MPa.m1/2 for comparable velocities in composites where the transformation does not occur (KIC=4.5 MPa.m1/2). This behavior is a result of crack‐tip shielding by the dissipation of strain energy in the transformation zone surrounding the crack. The stress corrosion parameter n is lower and A greater in these fine‐grained composite materials than in fine‐grained aluminas. This is a result of the residual tensile stresses associated with larger (≥1 μm) monoclinic ZrO2 particles which reside along the intergranular crack path.

This publication has 9 references indexed in Scilit: