AISI H13 Hot-Work Steel with Hard Chromium Plating Thermal Fatigue Behavior Evaluation
Authors:
- 21 November 2013
- journal article
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 849, 8-13
Abstract
A hard-coating on hot work tool steel can be used to obtain higher corrosion resistance, as well as better wear resistance. This study investigates the thermal fatigue performance of AISI H13 hot work tool steel with and without hard chromium plating. Treated specimens were characterized using microstructural analysis, X-ray diffraction analysis and microhardness measurement. The thermal fatigue test is based on cyclic induction heating and water cooling. The specimen was heated to the maximum surface temperature of 670°C followed with water injection to bring the specimen down to a minimum temperature of 25°C. The thermal fatigue testing in this study was conducted using 500 cycles. A vacuum heat treated specimen with a hardness of 47 HRC was used as the reference material. The hard chromium plated layer with a thickness 35 μm had a hardness of 930 HV0.1. The damage factor, defined as crack depth × crack width, of quenched and tempered H13 specimens and hard chromium plated specimens were 800 and 1760, respectively. The damage factor evaluation verified the vacuum heat treated specimen thermal fatigue resistance is superior to that of the hard chromium plated specimen.Keywords
This publication has 12 references indexed in Scilit:
- Thermal fatigue resistance of plasma sprayed yttria-stabilised zirconia onto borided hot work tool steel, bonded with a NiCrAlY coating: Experiments and modellingSurface and Coatings Technology, 2011
- Microstructural evolution during friction surfacing of tool steel H13Materials & Design (1980-2015), 2011
- Effect of cryogenic treatment on microstructure, mechanical and wear behaviors of AISI H13 hot work tool steelCryogenics, 2011
- The thermal fatigue resistance of vermicular cast iron coupling with H13 steel units by cast-in processMaterials & Design (1980-2015), 2010
- Thermal fatigue testing of Stellite 6-coated hot work tool steelMaterials Science and Engineering: A, 2010
- Influence of thermal homogenization treatment on structure and impact toughness of H13 ESR steelJournal of Iron and Steel Research International, 2009
- The effect of thermal fatigue on the hardness of hard chromium electroplatingsJournal of Materials Processing Technology, 2004
- Friction and wear behaviour prediction of HVOF coatings and electroplated hard chromium using neural computationMaterials Letters, 2004
- Effects of tungsten carbide thermal spray coating by HP/HVOF and hard chromium electroplating on AISI 4340 high strength steelSurface and Coatings Technology, 2001
- Residual stresses and crystallographic texture in hard-chromium electroplated coatingsSurface and Coatings Technology, 1997