Sustainable and cheaper energy storage devices are the key to the global decarbonizing initiative. The alarming consequences of mining metals like lithium are surmountable by transitioning towards alternatives like zinc-based energy storage and using greener components in the battery architecture. This work explores bacterial cellulose, a proven sustainable biomaterial made through microbial fermentation, as an electrode and electrolyte for a zinc ion battery. Combined with the simplicity and scalability of the preparation method for bacterial cellulose, we designed a tri-layer electrode with V 2 O 5 and nano-fibrillated hydrogel electrolyte for an all-solid-state zinc ion battery. The CNT-cellulose-based large-surface scaffolds encapsulating V 2 O 5 facilitate the manufacturing of inexpensive electrodes exhibiting a high capacity of 200 mAh g -1 at 4 A g -1 after 500 cycles with excellent stability. On the other hand, the hydrogel electrolyte offers a high ionic conductivity of 41 mS cm -1 at 30°C. The hydrogel is designed by a facile solvent exchange approach, where glycerol substitutes the free water molecules and settles between cellulose nanofibers. Owing to its bigger molecular size and ability to form hydrogen bonds with the cellulose fibers, a highly stable BC-based gel could be developed that regulates ion transport and extends the potential window compared to conventional hydrogels. Utilizing differential scanning calorimetry (DSC) to determine a eutectic phase of the water-glycerol mixture, we were also able to expand the operating temperature up to -40°C and investigate the performance of these zinc-ion batteries at sub-zero temperatures.