Study on the preparation of diamond-coated tools and their cutting performance using the segmented oxygen-doping method at low temperatures
- 1 January 2026
- journal article
- research article
- Published by Canadian Science Publishing in Transactions of the Canadian Society for Mechanical Engineering
- Vol. 50, 1-8
Abstract
The paper proposes a segmented oxygen-doping process technology and discusses and analyzes the surface morphology, quality, indentation morphology, and tool wear performance of diamond films. The results show that using the segmented oxygen-doping process (first low-temperature oxygen doping for 2 h, followed by high-temperature oxygen-free deposition for 9 h), the diamond morphology is uniform and clear, the residual stress of the diamond film is 0.674 GPa (about 53% of that of the high-temperature process), and the indentation crack diameter is about 312.7 µm. In addition, XRD peak intensity results show that the samples prepared by the segmented oxygen-doping process preferentially exhibit (111) and (110) orientations. The deposition reaction rate is increased to 3.64 µm/h (about 84% of the high-temperature process). The surface wear of diamond-coated tools is reduced to 92.0 µm, and the wear trend of the coated tools is lower than that of the low-temperature and high-temperature process wear curves, improving their wear resistance.Keywords
Funding Information
- Key Scientific Research Project of Colleges and Universities in Henan Province (25A590007)
- Key Scientific Research Project of Colleges and Universities in Henan Province (26A460026)
- Henan Provincial Science and Technology Research Project (242102210198)
- Henan Provincial Science and Technology Research Project (242102220045)
- Henan Provincial Science and Technology Research Project (252102220065)
- Henan Provincial Science and Technology Research Project (252102221025)
This publication has 26 references indexed in Scilit:
- HiPIMS fabricated Al, Cr doped multilayer diamond-like carbon coating for enhancing corrosion resistant of 9Cr18 stainless steels in marine environmentCeramics International, 2025
- Preparation of homogeneous SiC coating on diamond particles by magnetron sputtering for diamond/Al composites with high thermal conductivityCeramics International, 2025
- Investigation of a low-temperature-dominant HFCVD composite process for high-toughness diamond coated milling cutters in 5G-PCB applicationsJournal of Materials Research and Technology, 2025
- New method of electrochemical pretreatment for CVD diamond coating: Cobalt removal and polishing of cemented carbide toolsInternational Journal of Refractory Metals and Hard Materials, 2025
- Crystalline Si coating on diamond particles by silane CVD and the improving thermal conductivity of diamond-Si/Al compositesDiamond and Related Materials, 2025
- A tunable TiC coatings on diamonds using an innovative two-step molten salt strategyDiamond and Related Materials, 2025
- Enhanced wear resistance of CuSn19Ti10/Ni-coated diamond composite coatings prepared by laser cladding: Influence of nickel plating on diamond retention and microstructureInternational Journal of Refractory Metals and Hard Materials, 2025
- Fabrication, tribological properties and cutting performances of high-quality multilayer graded MCD/NCD/UNCD coated PCB end millsDiamond and Related Materials, 2021
- Growth of micro- and nanocrystalline dual layer composite diamond films by microwave plasma CVD: Influence of CO2 concentration on growth of nano-layerJournal of Crystal Growth, 2015
- Low temperature diamond growth by linear antenna plasma CVD over large areaPhysica Status Solidi (b), 2012