Evaluation of Temperature and Roughness Alteration of Diode Laser Irradiation of Zirconia and Titanium for Peri-Implantitis Treatment

Authors:

Abstract
Objective: This study investigated the effects of diode laser (gallium, aluminium, arsenide [GaAlAs]) irradiation with decontamination parameters on the temperature and roughness of yttrium-stabilized tetragonal zirconia polycrystal (Y-TZP), titanium (TI), and sandblasted large grit acid-etched titanium (SLA). Materials and methods: Three groups ( n = 10) of standardized disks with 5 mm diameter and 2 mm thickness were produced with Y-TZP obtained from computer-aided design and computer-aided manufacturing (CAD-CAM), machined TI and SLA. The diode laser single application (808 nm, 20 sec, 1 W, 50 Hz, t on = 100 ms, t off = 100 ms, energy density = 28.29 J/cm 2 ) was performed in contact mode, on each disk. The temperature was measured by a thermosensor attached to a digital thermometer fixed to the opposite irradiated surface. The temperature gradient (ΔT) was calculated (ΔT = final temperature – initial temperature) for each group. The parameters Ra (in μm) and Sa (in μm 2 ) were measured by white light confocal laser microscopy to express the surface roughness. Data of ΔT was statistically analyzed by one way ANOVA at the 95% confidence level and compared by Tukey post-hoc test (α = 0.05). Roughness data was analyzed by t test. Results: The diode laser irradiation presented the following results (ΔT value): Y-TZP = 10.3°C B ; TI = 38.6°C A , and SLA = 26.7°C A . The ΔT values ( ° C) of the titanium groups were higher than for the Y-TZP group. For both roughness parameters (Ra and Sa), data did not show statistical significant differences to “irradiation” factor ( p > 0.05) to Y-TZP and SLA. The Ra results (in μm) were: Y-TZP (control) = 0.73 (0.55); Y-TZP (irradiated) = 0.45 (0.27); SLA (control) = 0.74 (0.23); and SLA (irradiated) = 0.99 (0.33). The Sa results (in μm 2 ) were: Y-TZP (control) = 1.39 (1.05); Y-TZP (irradiated) = 0.73 (0.41); SLA (control) = 0.85 (0.08); and SLA (irradiated) = 1.27 (0.44). Conclusions: Diode laser irradiation for peri-implantitis treatment increased both zirconia and TI temperature without surface roughness alterations.

This publication has 24 references indexed in Scilit: