Abstract
CaGdAlO4 crystals doped with Ti ions were grown using the Czochralski technique in a reducing atmosphere in order to convert the valence of Ti to trivalence. The fluorescence of the 2E2T2 transition of Ti3+ in the crystals shows a broad band with a peak at 535 nm excited with the light of 410 nm in the optical absorption band at room temperature because of a strong electron-phonon coupling of the 2E excited state. The Ti3+ fluorescence is influenced in intensity by O2− vacancies at the ligands of the Ti3+ octahedra along the c axis, which are easily produced in a reducing atmosphere. The x-ray crystal analyses and the polarization of the optical absorption and fluorescence spectra deduce the energy levels and wave functions of the ground and excited states of Ti3+ in CaGdAlO4. The peak energy of the fluorescence band shifts to higher energy as increasing excitation energy in the absorption band. The linear dependence of the fluorescence-peak energy on the excitation energy shows that the fluorescence is inhomogeneously broadened by a random distribution of Ca2+ and Gd3+ ions in the disordered lattice.

This publication has 9 references indexed in Scilit: