Mineral Trioxide Aggregate as a Multicomponent Interfacial Layer for Dendrite-Free Lithium Metal Deposition

Authors:

Abstract
The practical application of Li-metal batteries is hindered by nonuniform Li deposition and continuous degradation of the solid electrolyte interphase (SEI). Here, commercially available mineral trioxide aggregate (MTA), a multicomponent calcium silicate-based dental material, was repurposed as a mineral-derived interfacial modifier for Cu current collectors. Structural and compositional analyses confirmed that MTA consists of agglomerated nanoscale particles containing multiple calcium silicate-based and other inorganic phases. Ex-situ SEM images show that the MTA layer promoted spatially distributed Li nucleation and more continuous and compact Li deposition, whereas bare Cu exhibited localized nucleation followed by nonuniform and dendritic growth. More importantly, XPS depth profiling revealed pronounced F enrichment throughout the interphase on MTA-coated Cu, including a persistent inorganic fluoride contribution, demonstrating the formation of an F-rich SEI at the MTA-modified interface. The combined regulation of Li deposition morphology and interphase chemistry suppressed localized dendritic growth and improved Li plating/stripping reversibility. At the current density of 0.5 mA cm‐2 for 1.0 mAh cm‐2, MTA-coated Cu maintained a Coulombic efficiency above 95% for 250 cycles, whereas bare Cu exhibited rapid deterioration after approximately 80 cycles. Improved cycling performance was also obtained at higher current densities of 1.0 and 2.0 mA cm‐2. These findings demonstrate that readily available multicomponent mineral materials can serve as dual physical and chemical interfacial modifiers for simultaneously regulating Li growth and SEI formation in Li-metal batteries.

This publication has 23 references indexed in Scilit: