Analysis of Recovery Characteristics and Parameter Dependence under Dishing in Cu/SiO₂ Interconnect Bonding Structures
- 8 June 2026
- journal article
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Components, Packaging and Manufacturing Technology
- Vol. PP (21563950) , 1
Abstract
As semiconductor device integration continues to scale, ensuring the reliability of Cu–Cu direct bonding has emerged as a critical requirement for next-generation three-dimensional integrated circuits (3D-ICs) and wafer-level packaging (WLP) technologies. However, dishing defects induced by chemical mechanical polishing (CMP) lead to non-uniform interfacial contact, thereby causing void formation, debonding, and overall degradation of bonding quality. In this work, we combine finite element simulations, XGBoost–SHAP-based machine-learning analysis, and experimental validation to quantitatively evaluate the influence of dishing gap size, bonding temperature, and applied pressure on interfacial recovery. The results revealed that smaller gaps exhibited higher recovery ratios, with temperature identified as the most dominant factor, followed by gap size and pressure as secondary contributors. Experimental validation was carried out using photolithography-based step-height patterns (1000 μm and 2000 μm). 3D profiler measurements indicated increased step height with larger patterns, while Scanning Acoustic Tomography (SAT) demonstrated that bonding yields above 99% could be achieved under high-temperature and high-pressure conditions, whereas significantly reduced bonding ratios were observed under lower conditions. The experimental results were in strong agreement with the simulations, and further analysis confirmed that when the dishing gap was ≤0.15 μm, stable bonding ratios above 80% could be consistently obtained at ~330–360 °C and 6–6.5 MPa. These results indicate that reliable Cu–Cu bonding does not necessarily require complete elimination of dishing; rather, maintaining the effective dishing gap at or below 0.15 μm and prioritizing temperature-driven recovery enables stable bonding above 80% under approximately 330–360 °C and 6–6.5 MPa for the investigated structure.Keywords
Funding Information
- National Research Foundation of Korea (RS-2023-00239657)
- National Research Foundation of Korea (RS-2024-00440244)
This publication has 27 references indexed in Scilit:
- Grain boundary motions of low temperature and low pressure copper to copper direct bonding by electroplating ultra-fine-grain (UFG) CuScientific Reports, 2025
- Review of Cu–Cu direct bonding technology in advanced packagingNanotechnology, 2025
- Low temperature Cu–Cu direct bonding in air ambient by ultrafast surface grain growthRoyal Society Open Science, 2024
- Integrated Process-Mechanical Stress Analysis of 2.5D/3D ICs with Two Types of Interconnections in Advanced Packaging2023
- Cu CMP Dishing Control for Fine Pitch Wafer-to-Wafer (W2W) Hybrid Bonding2022
- Enhancement of fatigue resistance by recrystallization and grain growth to eliminate bonding interfaces in Cu–Cu jointsScientific Reports, 2022
- In-Depth Parametric Study of Ar or N2 Plasma Activated Cu Surfaces for Cu-Cu Direct Bonding2021
- Thermomechanical finite element modeling of Cu–SiO2 direct hybrid bonding with a dishing effect on Cu surfacesInternational Journal of Solids and Structures, 2017
- A novel approach for forming ductile Cu-to-Cu interconnection2016
- Low-temperature direct copper-to-copper bonding enabled by creep on (111) surfaces of nanotwinned CuScientific Reports, 2015