Environmental Effects on Oxide/Oxide Composites
- 26 September 2014
- book chapter
- Published by Wiley
- p. 293-333
Abstract
No abstract availableKeywords
This publication has 66 references indexed in Scilit:
- Effects of Steam Environment on Creep Behavior of Nextel™610/Monazite/Alumina Composite at 1,100°CApplied Composite Materials, 2009
- Creep of Nextel™720/alumina–mullite ceramic composite at 1200°C in air, argon, and steam☆Composites Science and Technology, 2009
- Creep behavior in interlaminar shear of Nextel™720/alumina ceramic composite at elevated temperature in air and in steamComposites Science and Technology, 2008
- Effects of frequency and environment on fatigue behavior of an oxide–oxide ceramic composite at 1200°CInternational Journal of Fatigue, 2008
- Assessments of Life Limiting Behavior in Interlaminar Shear For Hi‐Nic SiC/SiC Ceramic Matrix Composite at Elevated Temperature2007
- Compressive creep behavior of an oxide–oxide ceramic composite with monazite fiber coating at elevated temperaturesMaterials Science and Engineering: A, 2007
- Load-rate dependency of ultimate tensile strength in ceramic matrix composites at elevated temperaturesInternational Journal of Fatigue, 2005
- Advanced ceramic matrix composite materials for current and future propulsion technology applicationsActa Astronautica, 2004
- Creep Rupture Behavior of±45° Oxide/Oxide Nextel™ 720/AS Composite2003
- Hydrogen defects in α-Al2O3 and water weakening of sapphire and alumina ceramics between 600 and 1000°C—I. Infrared characterization of defectsActa Materialia, 2000