Effect of Heat Treatments on the Crack‐Healing and Static Fatigue Behavior of Silicon Carbide Sintered with Sc 2 O 3 and AlN
- 30 August 2005
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 88 (12) , 3478-3482
Abstract
Crack‐healing behavior of silicon carbide ceramics sintered with AlN and Sc 2 O 3 has been studied as a function of heat‐treatment temperature and applied stress. Results showed that heat treatment in air could significantly increase the indentation strength whether a stress is applied or not. After heat treatment with no applied stress at 1300°C for 1 h in air, the indentation strength of the specimen with an indentation crack of ∼100 μm (≈2c) recovered its strength fully at room temperature. In addition, a simple heat treatment at 1200°C for 5 h under an applied stress of 200 MPa in air resulted in a complete recovery of the unindented strength at the healing temperature. However, higher applied stress led to fracture of the specimens during heat treatment. The static fatigue limit of the specimens crack healed at 1200°C for 5 h under 200 MPa was ∼450 MPa at the healing temperature. The ratio of the static fatigue limit of the crack‐healed specimen to the unindented strength was ∼80%.Keywords
This publication has 23 references indexed in Scilit:
- Crack-healing behavior and resultant strength properties of silicon carbide ceramicJournal of the European Ceramic Society, 2005
- High‐Temperature Fatigue Strength of Crack‐Healed Al2O3Toughened by SiC WhiskersJournal of the American Ceramic Society, 2004
- Intergranular glassy phase free SiC ceramics retains strength at 1500 °CScripta Materialia, 2004
- Crack-healing behavior and static fatigue strength of Si3N4/SiC ceramics held under stress at temperature (800, 900, 1000 °C)Journal of the European Ceramic Society, 2003
- Effect of crack-healing and proof-testing procedures on fatigue strength and reliability of Si3N4/SiC compositesJournal of the European Ceramic Society, 2003
- High-temperature effects in the fracture mechanical behaviour of silicon carbide liquid-phase sintered with AlN–Y2O3 additivesJournal of the European Ceramic Society, 2001
- High temperature mechanical behaviour of liquid phase sintered silicon carbideJournal of the European Ceramic Society, 1998
- Crack healing in silicon nitride and alumina ceramicsJournal of Materials Science Letters, 1996
- DAMAGE HEALING AND STRENGTHENING BEHAVIOUR IN INTELLIGENT MULLITE/SiC CERAMICSFatigue & Fracture of Engineering Materials & Structures, 1995
- Crack healing behavior of hot pressed silicon nitride due to oxidationScripta Metallurgica et Materialia, 1992