Influence of Environmental Factors on Corrosion in CO2 Source Well

Authors:

Abstract
The effect of H2S and O2 on CO2 corrosion of pure iron and Cr steels was experimentally and theoretically investigated. From the viewing point of contamination in the CO2 source well, both a little amount of H2S and O2 were examined mainly by the autoclave tester and the solution loop tester. A contamination of H2S plays two conflicting roles on the Types 1 - and 2-CO2 corrosion behaviors of pure iron. One is the accelerating effect on cathodic reaction and the other is the suppressive effect of corrosion rate owing to forming a temporary FeS film. The cathodic reaction is accelerated even in the low concentration of H2S such as 3.3 ppm. The temporary FeS film formation occurs even in the relatively low concentration of H2S, where FeCO3 should be a main corrosion product in the equilibrium conditions. Such a film formation is due to the kinetics of localized dissolution rate of iron. Therefore, the higher the concentration of H2S and the higher temperature, the more the suppressive effect on CO2 corrosion. The Type 3-CO2 corrosion at the temperature over 150°C is very similar to the manner of pure CO2 corrosion, because FeCO3 is formed more easily than FeS. The effect of H2S on CO2 corrosion of Cr steels is significantly detrimental to the resistance to CO2 corrosion owing to the initiation of pitting corrosion, because H2S could decrease the over potential of reduction of H+ ion. The field experience in the Tuscaloosa Trend is presented to ascertain the correlation with the laboratory data. O2 contamination up to 1670 ppm increases a corrosion rate of pure ion through the activation of cathodic reaction with increasing O2 concentration. O2 contamination has a tendency to increase a susceptibility to pitting corrosion of Cr steel in the CO2 environment. In the present work, the pitting corrosion in 25% Cr steel was observed in the condition of 1670 ppm O2 at 80°C. Joining itself to cathodic reaction is a cause of raising corrosion potential and initiating pitting corrosion.