Strength Effect in Stress Corrosion Cracking of High-Strength Steel in Aqueous Solution

Authors:
  • KGK.W. Gao
    K.W. Gao
  • LQL.J. Qiao
    L.J. Qiao
  • YWY.B. Wang
    Y.B. Wang

Abstract
The threshold stress intensity (KISCC) of stress corrosion cracking (SCC) for 40CrMo steel in 3.5% sodium chloride (NaCl) solution decreased exponentially with the increase in the yield strength, σys (i.e., KISCC = 1.38 × 106exp[–8.26 × 10–3σys]). The threshold stress intensity of hydrogen-induced cracking (KIH) during dynamical charging for 40CrMo steel decreased linearly with the logarithm of the concentration of diffusible hydrogen, C0 (i.e., KIH = 31.3 – 9.1 lnC0). This equation was also applicable to SCC of the high-strength steel in aqueous solution. The critical hydrogen enrichment concentration (Cth) necessary for SCC of high-strength steel in water, decreased exponentially with the increase in the σys. Based on the result, the relationship between KISCC and σys could be deduced as KISCC = aκ1exp(–κ2σys), where a=3RTπρ/2(1+ν)V¯H, and κ1 and κ2 depended upon the compositions and microstructure of the steel as well as the test conditions.

This publication has 12 references indexed in Scilit: