Deposition of boron on fuel rod surface under sub-cooled boiling conditions—An approach toward understanding AOA occurrence
Authors:
- Shunsuke UchidaSUShunsuke Uchida
- Yamato AsakuraYAYamato Asakura
- Hiroaki SuzukiHSHiroaki Suzuki
- 1 July 2011
- journal article
- Published by Elsevier in Nuclear Engineering and Design
- Vol. 241 (7) , 2398-2410
Abstract
No abstract availableKeywords
This publication has 15 references indexed in Scilit:
- Evidence of Ni2FeBO5 and m-ZrO2 precipitates in fuel rod deposits in AOA-affected high boiling duty PWR coreJournal of Nuclear Materials, 2008
- Deposition of Nickel and Cobalt Ions on Heated Surface under Nucleate Boiling ConditionJournal of Nuclear Science and Technology, 1989
- Deposition of nickel and cobalt ions on heated surface under nucleate boiling condition.Journal of Nuclear Science and Technology, 1989
- Chemical state and deposition rate of nickel ion deposit produced on heated surface in high pressure boiling water.Journal of Nuclear Science and Technology, 1988
- In situ thickness measurement of nickel ion deposits on heated surface in water by thermal wave methods.Journal of Nuclear Science and Technology, 1988
- Noncontact Measurement of Film Thickness by the Photothermal Deflection MethodJapanese Journal of Applied Physics, 1987
- Iron Oxide Deposition on Heated Surfaces in Pressurized Boiling WaterNuclear Science and Engineering, 1979
- Deposition of Iron Oxide on Heated Surfaces in Boiling WaterNuclear Science and Engineering, 1978
- A Consideration on the Relation between Laminar Flame Speed and Ignition DelayTransactions of the Japan Society of Mechanical Engineers, 1973
- Thermodynamic Effects on Desinent Cavitation on Hemispherical Nosed Bodies in Water at Temperatures From 80 Deg F to 260 Deg FJournal of Basic Engineering, 1970