Fracture load and failure types of different veneered polyetheretherketone fixed dental prostheses
Authors:
- 15 March 2016
- journal article
- research article
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 20 (9) , 2493-2500
Abstract
Objective The aim of this study is to investigate the fracture load of different veneered PEEK 3-unit fixed dental prosthesis (FDPs) after different aging regimens. Methods Congruently anatomically shaped 3-unit FDPs were milled using a master stl-data set and randomly divided into four groups (N = 120, n = 30 per veneering group), which were veneered using different veneering methods: (i) digital veneering with breCAM.HIPC, (ii) conventional veneering with crea.lign, (iii) conventional with crea.lign paste, and (iv) using pre-manufactured veneers visio.lign. The FDPs were then adhesively cemented on a metal abutment and fracture loads were measured in a universal testing machine (1 mm/min) before and after aging (10,000 thermal cycles, 5/55 °C). Two- and one-way ANOVA followed by post hoc Scheffé tests were used for data analysis (p < 0.05). Results This investigation showed an influence of the veneering method on the fracture load results independent of the aging level. The highest fracture load was measured for the FDPs with digital veneering (1882 ± 152 N at baseline, 2021 ± 184 N after thermocycling). The remaining groups showed comparable results, and no impact of thermal aging was observed. Digital and conventional veneers showed cracks in the pontic region starting from the connector area as a main failure type after loading, while the pre-manufactured veneers showed predominantly adhesive failures. Conclusions The digital veneering method showed the highest fracture load resistance. Thermal aging showed no impact on the fracture load of all tested veneered PEEK 3-unit FDPs. Clinical relevance According to this study results, reliable veneering of PEEK FDPs can be achieved with digital veneering.Keywords
This publication has 24 references indexed in Scilit:
- Impact of plasma treatment of PMMA-based CAD/CAM blanks on surface properties as well as on adhesion to self-adhesive resin composite cementsDental Materials, 2013
- Polyetheretherketone-A suitable material for fixed dental prostheses?Journal of Biomedical Materials Research Part B: Applied Biomaterials, 2013
- Influence of plasma pretreatment on shear bond strength of self-adhesive resin cements to polyetheretherketoneClinical Oral Investigations, 2013
- Influence of surface conditioning on bonding to polyetheretherketon (PEEK)Dental Materials, 2012
- The improvement of adhesive properties of PEEK through different pre-treatmentsApplied Surface Science, 2012
- Load-bearing capacity of CAD/CAM milled polymeric three-unit fixed dental prostheses: Effect of aging regimensClinical Oral Investigations, 2012
- Effect of different surface pre-treatments and luting materials on shear bond strength to PEEKDental Materials, 2010
- PEEK biomaterials in trauma, orthopedic, and spinal implantsBiomaterials, 2007
- Polyetheretherketone as a biomaterial for spinal applicationsBiomaterials, 2006
- Bite force and state of dentitionActa Odontologica Scandinavica, 1977