Abstract
When heating rate was higher than 0.5 K/min until debinding temperature, a bloating of thermoplastic binder inside the injection molded ceramic core was occurred due to abrupt evaporation. Therefore, bloating of surface in the sintered specimen could be controlled by applying slow heating rate at 0.2 K/min.