Microstructure and mechanical properties of Wire Arc Additive Manufactured (WAAM) Inconel 718 parts via post heat treatments
Authors:
- Zhe ChenZCZhe Chen
- Gim Song SohGSGim Song Soh
- 17 October 2022
- journal article
- research article
- Published by Elsevier in Materials Today: Proceedings
- Vol. 70, 567-573
Abstract
No abstract availableFunding Information
- NAMIC (2020017)
- Agency for Science Technology and Research (A19E1a0097)
This publication has 13 references indexed in Scilit:
- Microstructural evolution and mechanical properties of Inconel 718 superalloy thin wall fabricated by pulsed plasma arc additive manufacturingJournal of Alloys and Compounds, 2020
- Wire Arc Additive Manufacturing (WAAM) process of nickel based superalloys – A reviewMaterials Today: Proceedings, 2020
- Wire + Arc Additively Manufactured Inconel 718: Effect of post-deposition heat treatments on microstructure and tensile propertiesMaterials & Design, 2019
- Investigation of process factors affecting mechanical properties of INCONEL 718 superalloy in wire + arc additive manufacture processJournal of Materials Processing Technology, 2019
- Enhancing mechanical properties of wire + arc additively manufactured INCONEL 718 superalloy through in-process thermomechanical processingMaterials & Design, 2018
- Optimising the mechanical properties of Ti-6Al-4V components produced by wire + arc additive manufacturing with post-process heat treatmentsJournal of Alloys and Compounds, 2018
- Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: Sample orientation dependence and effects of post heat treatmentsMaterials Science and Engineering: A, 2018
- Impact of heat treatment on mechanical behaviour of Inconel 718 processed with tailored microstructure by selective laser meltingMaterials & Design, 2017
- Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloyMaterials Science and Engineering: A, 2015
- Aging of the Inconel 718 alloy between 500 and 750 °CJournal of Materials Research, 1997