Effect of Cu/Fe Mass Ratio on Chemical Looping Combustion Performance of Bayan Obo Iron Concentrate‐Based Cu‐Fe Composite Oxygen Carriers

Authors:

Abstract
In order to explore efficient oxygen carriers (OCs) for chemical looping combustion (CLC), this article investigates Bayan Obo iron concentrate‐based Cu‐Fe composite OCs with varying Cu/Fe mass ratios (1:1, 1:1.5, 1:2) for CLC performance using thermogravimetric analysis (temperature‐programmed reduction (TPR), isothermal reduction, redox cycling) and characterization (Brunauer–Emmett–Teller (BET), X‐ray diffraction (XRD), scanning electron microscopy (SEM)). The TPR tests reveal a three‐stage reduction pathway of CuFe 2 O 4 with CO: CuFe 2 O 4 → Cu + Fe 3 O 4 → FeO → Fe. The 1:1 Cu/Fe ratio OCs exhibit good reducibility, with a 4.32% higher mass loss than raw iron concentrate, lower mass‐loss commencing temperature than other ratios (280°C), higher oxygen release than other ratios above 806°C under N 2 , which intensifies with temperature, and high kinetic activity (always the first to reach equilibrium in isothermal reduction test). In 11 thermogravimetric redox cycles, the 1:1 Cu/Fe ratio sample maintains high reduction conversion, showing a maximum mass loss difference of 5.09% compared to the iron concentrate. Its stable mass loss over the initial seven cycles demonstrates its good cycling stability.
Funding Information
  • Education Department of Inner Mongolia Autonomous Region (NO. NJZZ23061)

This publication has 22 references indexed in Scilit: