Abstract
A refractory silicon nitride joint, which contains β–Si3N4 grains and grain boundary amorphous phase in the joined layer, was developed with the aid of a ceramic adhesive based on the system Si3N4–Y2O3–SiO2–Al2O3. The similarity in chemistry and microstructure between the parent ceramic and the joint zone indicates that the joining mechanism is the same as that involved in the sintering of Si3N4. The resultant joint exhibits a high bond strength of 550 MPa at 25 °C and retains a strength of 332 MPa at 1000 °C. Post-joining hot-isostatic pressing was applied to strengthen the joint, resulting in increased strengths of 668 MPa at room temperature and 464 MPa at 1000 °C.Keywords
This publication has 28 references indexed in Scilit:
- Silicon nitride joining using rare-earth reaction sinteringScripta Materialia, 1997
- Evaluation of Brazed Silicon Nitride Joints: Microstructure and Mechanical PropertiesJournal of the American Ceramic Society, 1996
- An evaluation of the partial transient liquid phase bonding of Si3N4 using Au coated Ni22Cr foilsActa Materialia, 1996
- Interfaces of polymeric precursors with ceramics/metalsScripta Metallurgica et Materialia, 1994
- Joining SiAlON Ceramics Using Composite β‐SiAlON–Glass AdhesivesJournal of the American Ceramic Society, 1992
- Mechanistic Analysis of Time‐Dependent Failure of Oxynitride Glass‐Joined Silicon Nitride below 1000°CJournal of the American Ceramic Society, 1991
- Partial transient liquid-phase metals layer technique of ceramic-metal bondingJournal of Materials Science Letters, 1991
- Bonding Mechanisms in Silicon Nitride BrazingJournal of the American Ceramic Society, 1990
- Sinter and sinter-HIP of silicon nitride ceramics with yttria and alumina additionsJournal of Materials Science, 1989
- Mechanical Behavior of Ceramic-Metal Braze Joints1989