Hydride Phases in Austenitic Stainless Steels
Authors:
- 1 October 1979
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 35 (10) , 461-464
Abstract
Electrolytic charging of austenitic stainless steels with hydrogen induces formation of two distinct alloy hydride phases, both being unstable under normal atmospheric conditions. One of the new phases denoted Hγ, has the same Bravais lattice as austenite (fcc), whereas another, denoted Hϵ, exhibits an hcp structure. Compared with hydrogen-free austenite and ϵ-martensite, respectively, the lattice constants of hydride phases are larger by about 5%. During charging of austenitic stainless steels with hydrogen evolved electrolyticaily from promoter containing acid solutions, these hydrides form a hard and brittle surface layer, several μm thick with numerous microcracks, and it is probable that these hydride phases play an important role during stress corrosion cracking (SCC) of austenitic stainless steels.Keywords
This publication has 8 references indexed in Scilit:
- An X-ray Study of Hydrides Formed in Austenitic Stainless SteelsTransactions of the Iron and Steel Institute of Japan, 1978
- Hydride formation in nickel-iron alloysJournal of Physics and Chemistry of Solids, 1971
- Hydrogen-Induced Phase Transformations in Type 304L Stainless SteelsCorrosion, 1968
- Hydrogen Embrittlement of Austenitic Stainless SteelCorrosion, 1965
- Relationship Between Hydrogen Pickup and Susceptible Paths in Stress Corrosion Cracking of Type 304 Stainless SteelCorrosion, 1963
- The hydrogen atom positions in face centered cubic nickel hydrideJournal of Physics and Chemistry of Solids, 1963
- Struktur der im Nickel bei elektrolytischer Beladung entstehenden wasserstoffreichen PhaseThe Science of Nature, 1960
- Neutron-diffraction observations on the palladium-hydrogen and palladium-deuterium systemsJournal of Physics and Chemistry of Solids, 1957