The Atmospheric corrosion of statue bronzes exposed to SO2and NO2
Authors:
- 1 November 1997
- journal article
- corrosion science-and-technology
- Published by Wiley in Materials and Corrosion
- Vol. 48 (11) , 721-730
Abstract
We report on the atmospheric corrosion of different cast statue bronzes in humid air containing ppb levels of SO2and SO2+NO2. In addition, copper, tin, zinc, and lead samples were studied in these environments. The samples were exposed to synthetic atmospheres with careful control of pollutant concentrations, relative humidity and flow conditions. Deposition of SO2was studied using on‐line gas analysis. The weight gain was registered after four weeks exposure, and corrosion products were analysed by Electron Probe Micro Analyser (EPMA), X‐ray diffraction (XRD), and Fourier Transform Infrared spectroscopy (FTIR).The synergistic effect of SO2and NO2was remarkable on all bronze materials examined. The weight gain was correlated to alloy composition. Thus, high zinc and low lead content resulted in the greatest weight gain, while high tin content favoured a low weight increase. Lead exhibited a rapid deposition of SO2followed by zinc and copper, while tin was unreactive towards SO2. There was no measurable indication that microstructure influenced corrosion.The corrosion product morphology found in SO2+NO2environment indicated a localised type of attack. The anodic sites were covered by a tin‐rich corrosion product close to the metal. Oxidation of soluble divalent tin by O2at the anodic sites to form insoluble SnO2– xH2O, is suggested to explain the corrosion protection afforded by alloying with tin. Tin was enriched in the corrosion products while no lead was found. The zinc/copper relation was higher in the corrosion products than in the alloy composition.Keywords
This publication has 10 references indexed in Scilit:
- The Formation of Black Patina on Copper in Humid Air Containing Traces of SO 2Journal of the Electrochemical Society, 1997
- Corrosion of bronze by acetic and formic acid vapours, sulphur dioxide and sodium chloride particlesMaterials and Corrosion, 1995
- Structure of Cu2.5(OH)3SO4.2H2O: a Novel Corrosion Product of Copper.Acta Chemica Scandinavica, 1995
- Chemical Mechanisms for the Atmospheric Corrosion of LeadJournal of the Electrochemical Society, 1994
- A Laboratory Study of the Effect of Ozone, Nitrogen Dioxide, and Sulfur Dioxide on the Atmospheric Corrosion of ZincJournal of the Electrochemical Society, 1993
- A laboratory study of corrosion reactions on statue bronzeCorrosion Science, 1993
- Initial Stages of Copper Corrosion in Humid Air Containing SO 2 and NO 2Journal of the Electrochemical Society, 1993
- Degradation of monumental bronzesAtmospheric Environment. Part B. Urban Atmosphere, 1992
- Atmospheric Corrosion Tests of Copper and Copper Alloys in Sweden—16-Year Results1982
- Korrosionsschäden an BronzeplastikenMaterials and Corrosion, 1972