Abstract
To investigate the physical origin of high dielectric CaCu3Ti4.0O12 (CCTO), we have prepared the Ti-deficiency CaCu3Ti3.9O12 (CCTO39) ceramics, using the traditional solid state reaction method. Raman spectroscopy shows the damping of Fg(3) mode, i.e. the O-Ti-O antistretching motion, is higher in CCTO39 than in CCTO and suggests that the antistretching motion may be over damped in the CCTO39 samples. The dielectric spectrum presents that, the relative dielectric constant, ε′, reduces from ∼ 105 (CCTO) to ∼ 103 (CCTO39) above 150 K, and at the lowest temperature it reduces from ∼ 220 (CCTO) to ∼ 140 (CCTO39). The dissipation peaks are 10-foldly depressed. Their characteristic relaxation frequencies may not obey the Arrhenius law but a tentative relation. All the experiments suggest that the dielectric relaxation is related to the mutually correlated motion of Ti ions and defects.Keywords
This publication has 11 references indexed in Scilit:
- Effects of Cu stoichiometry on the microstructures, barrier-layer structures, electrical conduction, dielectric responses, and stability of CaCu3Ti4O12Acta Materialia, 2006
- Direct current bias effects on grain boundary Schottky barriers in CaCu3Ti4O12Applied Physics Letters, 2006
- Structurally frustrated relaxor ferroelectric behavior inPhysical Review B, 2005
- Clues to the Giant Dielectric Constant of CaCu3Ti4O12 in the Defect Structure of “SrCu3Ti4O12”Chemistry of Materials, 2004
- Nonintrinsic origin of the colossal dielectric constants inPhysical Review B, 2004
- Raman spectroscopy ofPhysical Review B, 2002
- Origin of apparent colossal dielectric constantsPhysical Review B, 2002
- Optical Response of High-Dielectric-Constant Perovskite-Related OxideScience, 2001
- Giant dielectric constant response in a copper-titanateSolid State Communications, 2000
- High Dielectric Constant in ACu3Ti4O12 and ACu3Ti3FeO12 PhasesJournal of Solid State Chemistry, 2000