Disorder effect on the magnetic behavior of mechanically alloyedFe1−xAlx(0.2⩽x⩽0.4)

Authors:

Abstract
We report on the magnetic properties of Fe1−xAlx alloys (0.2⩽x⩽0.4) produced by mechanical alloying by milling pure element powders for t=12, 24, and 36h. The alloys present a bcc lattice with compositional disorder and are ferromagnetic at room temperature, independently of the milling time. The lattice parameter of the x=0.2 sample presents a small decrease with t, whereas those of the x=0.3 and 0.4 samples remain constant independently of the milling time. The magnetic properties of the alloys with x=0.2 and 0.3 do not show important variations with t, while those of x=0.4 are strongly dependent on the milling time. For this latter alloy it was found that: (i) despite being the most diluted of the series, it presents a well developed ferromagnetic order at room temperature as the Mössbauer and hysteretic data have shown; (ii) the temperature dependence of the ac susceptibility and the Mössbauer spectra recorded at different temperatures evidence the occurrence of reentrant spin-glass and superparamagnetic phenomena. The enhancement of the ferromagnetic behavior and the presence of reentrant spin-glass freezing temperature and of a superparamagnetic blocking process are interpreted in terms of a simple localized model based on the disorder present in that alloy and on the occurrence of competitive interactions, namely, the ferromagnetic nearest-neighbor Fe-Fe interactions and the antiferromagnetic near-nearest-neighbor Fe-Fe ones. Taken together, these results evidence that the stabilization of the magnetic order takes place in the x=0.4 sample exclusively through the induction of compositional disorder and without any contribution from the lattice expansion.

This publication has 30 references indexed in Scilit: