Comparison of Uniaxial and Biaxial Strengths for Test Pieces with Controlled Flaws
Authors:
- 1 February 1982
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 65 (2) , C‐31
Abstract
Indentation cracks are used as controlled flaws in soda‐lime glass specimens for failure tests in uniaxial and biaxial loading. The inert strength is independent of loading type within the scatter of data. This result is discussed in relation to the conclusions of other workers who have reported systematic differences in similar comparative tests on specimens containing natural flaws.Keywords
This publication has 10 references indexed in Scilit:
- Biaxial Fracture Studies of a Glass‐CeramicJournal of the American Ceramic Society, 1981
- Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack SystemJournal of the American Ceramic Society, 1980
- Flaw Characteristics in Dynamic Fatigue: The Influence of Residual Contact StressesJournal of the American Ceramic Society, 1980
- Biaxial and Uniaxial Data for Statistical Comparisons of a Ceramic's StrengthJournal of the American Ceramic Society, 1979
- Residual stress effects in sharp contact crackingJournal of Materials Science, 1979
- Mixed‐Mode Fracture in Soda‐Lime GlassJournal of the American Ceramic Society, 1979
- Subcritical Crack Growth in Glass-Ceramics1978
- Mixed‐Mode Fracture from Controlled Surface Flaws in Hot‐Pressed Si 3 N 4Journal of the American Ceramic Society, 1976
- Indentation fracture: principles and applicationsJournal of Materials Science, 1975
- Microfracture beneath point indentations in brittle solidsJournal of Materials Science, 1975