Percolative Mechanism of Aging in Zirconia‐Containing Ceramics for Medical Applications
- 17 March 2003
- journal article
- research article
- Published by Wiley in Advanced Materials
- Vol. 15 (6) , 507-511
Abstract
For biomedical applications, zirconia‐toughened alumina ceramics (see Figure) would be very appropriate materials, provided that the zirconia content is kept below the percolation threshold (upper limit of 16 vol.‐% 3Y‐TZP inside an alumina matrix). That the concept of a percolation threshold is relevant when talking about aging degradation, is demonstrated by comparing specular IR reflectance measurements with aging experiments.Keywords
All Related Versions
This publication has 14 references indexed in Scilit:
- Mixed oxides prosthetic ceramic ball heads. Part 3: effect of the ZrO2 fraction on the wear of ceramic on ceramic hip joint prostheses. A long-term in vitro wear studyBiomaterials, 2001
- Mixed-oxides prosthetic ceramic ball heads. Part II: effect of the ZrO2 fraction on the wear of ceramic on ceramic jointsBiomaterials, 1999
- Low‐Temperature Aging of Y‐TZP CeramicsJournal of the American Ceramic Society, 1999
- Aging behavior of tetragonal zirconia polycrystal (TZP) ceramics in the temperature range of 200°C to 350°C in airScripta Materialia, 1999
- Role of H2O on the degradation process of Y-TZPJournal of Materials Science Letters, 1987
- Scaling theory of percolation clustersPhysics Reports, 1979
- Critical Behaviour of Conductivity and Dielectric Constant near the Metal‐Non‐Metal Transition ThresholdPhysica Status Solidi (b), 1976
- Percolation and ConductionReviews of Modern Physics, 1973
- Phase Analysis in Zirconia SystemsJournal of the American Ceramic Society, 1972
- Infrared Lattice Vibrations and Dielectric Dispersion in CorundumPhysical Review B, 1963