Electromigration in eutectic SnPb solder lines
Authors:
- 15 April 2001
- journal article
- conference paper
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 89 (8) , 4332-4335
Abstract
We have prepared eutectic SnPb solder lines for electromigration study by a process of solder reflow into V-grooves etched on (001) Si wafer surfaces. They are thick lines and are highly reproducible. We report here results of lines of 100 μm in width and 150 to 800 μm in length, stressed by a current density of at in ambient. The accumulation of a large lump of solder, rather than hillocks of Sn and Pb, was observed at the anode, and depletions and voids were observed at the cathode. By measuring the volume of the lump, we have calculated the average effective charge number of electromigration in the eutectic solder to be 33, which is close to the reported value of 47 for self-electromigration in bulk Pb. Using x-ray dispersive analysis, we found that Pb is the dominant diffusing species.
Keywords
This publication has 12 references indexed in Scilit:
- 1.55 μm reflection-type optical waveguide switch based on SiGe/Si plasma dispersion effectApplied Physics Letters, 1999
- Interface diffusion in eutectic Pb–Sn solderActa Materialia, 1998
- Reactive flow of molten Pb(Sn) alloys in Si grooves coated with Cu filmPhysical Review E, 1998
- Copper interconnections and reliabilityMaterials Chemistry and Physics, 1998
- The Flow of Liquids in Surface GroovesLangmuir, 1996
- Electromigration in metalsReports on Progress in Physics, 1989
- Diffusion of Sn in Pb to 30 kbarPhysical Review B, 1977
- Diffusion of , , , and in tinPhysical Review B, 1974
- Current-induced marker motion in gold wiresJournal of Physics and Chemistry of Solids, 1961
- The Dynamics of Capillary FlowPhysical Review B, 1921