Preliminary study of interfacial shear strength between PMMA precoated UHMWPE acetabular cup and PMMA bone cement
- 2 April 2003
- journal article
- research article
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 65B (2) , 272-279
Abstract
Followed by successful demonstration of high interfacial tensile strength in a new design of cemented all‐polyethylene acetabular cup, interfacial shear strength was investigated in this study, with the use of canine‐size prototypes of polymethylmethacrylate (PMMA) precoated UHMWPE acetabular cups. In addition to the PMMA precoated prototypes, three different types of controls were also prepared and tested: grooved UHMWPE cups, PMMA (bone cement) cups, and noncoated, plain UHMWPE cups. The interfacial shear strength of the precoated prototypes was 10.1 ± 0.69 MPa (n = 6), whereas it was 24.3 ± 0.78 MPa (n = 2) for the PMMA cup, 6.95 ± 0.21 MPa (n = 2) for the grooved UHMWPE cup, and 0.34 ± 0.47 MPa (n = 2) for the UHMWPE cup. These results indicate benefits of the PMMA precoating to stabilize the polyethylene acetabular cup securely when applied with bone cement in simulated clinical applications. Analysis of the failed PMMA precoated UHMWPE prototype cups suggested that the chemically induced bonds between precoated PMMA layer and bone cement played a key role in developing high shear strength. After the interfacial shear test of the PMMA precoated prototypes, major disruptions at the interface between treated UHMWPE and precoated PMMA layer were observed by scanning electron microscopy (SEM), which was a unique failure pattern, not found with other prototypes. © 2003 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 65B: 272–279, 2003Keywords
This publication has 18 references indexed in Scilit:
- Total Knee Arthroplasty With 4.4 mm of Tibial PolyethyleneClinical Orthopaedics and Related Research, 2001
- Effects of fatigue loading and PMMA precoating on the adhesion and subcritical debonding of prosthetic-PMMA interfacesJournal of Biomedical Materials Research, 2000
- Interfacial strength of compression-molded specimens between PMMA powder and PMMA/MMA monomer solution-treated ultra-high molecular weight polyethylene (UHMWPE) powderJournal of Biomedical Materials Research, 2000
- Mixed‐mode fracture toughness of the cobalt‐chromium alloy/polymethlymethacrylate cement interfaceJournal of Orthopaedic Research, 1999
- Precoating of ultrahigh molecular weight polyethylene with polymethylmethacrylate: Interfacial strengthJournal of Biomedical Materials Research, 1998
- The Mechanism of Loosening of Cemented Acetabular Components in Total Hip ArthroplastyClinical Orthopaedics and Related Research, 1992
- Thin film PMMA precoating for improved implant bone–cement fixationJournal of Biomedical Materials Research, 1982
- Intramedullary fixation of artificial hip joints with bone cement‐precoated implants. I. Interfacial strengthsJournal of Biomedical Materials Research, 1982
- Fracture of polyethylene acetabular cups. Report of two cases.Journal of Bone and Joint Surgery, 1979
- Some Physical and Mechanical Factors Affecting the Simple Shear Strength of MethylmethacrylateClinical Orthopaedics and Related Research, 1975