Analysis on peculiar fatigue fracture behaviour of shot peened metal using new threshold stress intensity factor range equation
- 20 October 2020
- journal article
- research article
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 44 (2) , 306-316
Abstract
A shot‐peened specimen with a precrack exhibits the following peculiar fatigue fracture behaviour. (1) Precracks can be rendered harmless by peening, even though the precrack reduced the fatigue limit by approximately 20%–60% of the nonpeened specimen. (2) When shot‐peened specimens were fractured at a higher stress than the fatigue limit, most specimens were fractured from outside the precracked part. (3) In most run‐out specimens, stage II (tensile type) nonpropagating cracks were observed. Why were nonpropagating cracks initiated and arrested? To explain the above fatigue behaviours, a new threshold stress intensity factor range ( ) equation is necessary. In this paper, a equation as a function of crack size was proposed using a nonlinear zone size criterion. By using the equation, the above peculiar fatigue fracture behaviours (1) and (2) and the stage II nonpropagating crack arrest condition could be evaluated quantitatively. Stage II nonpropagating crack initiation could be explained by considering the microdistribution of residual stress due to peening.Keywords
This publication has 21 references indexed in Scilit:
- Quantitative relationship between weld defect characteristic and fatigue crack initiation life for high-cycle fatigue propertyInternational Journal of Fatigue, 2019
- A Study on the Unification of the Threshold Stress Intensity Factor for Micro Crack GrowthTransactions of Japan Society of Spring Engineers, 2019
- Fatigue life prediction based on an equivalent initial flaw size approach and a new normalized fatigue crack growth modelEngineering Failure Analysis, 2016
- High- and very high-cycle plain fatigue resistance of shot peened high-strength aluminum alloys: The role of surface morphologyInternational Journal of Fatigue, 2015
- Evaluation of Acceptable Defect Size by Shot Peening Based on Fracture MechanicsTransactions of Japan Society of Spring Engineers, 2010
- PROCESS ZONE SIZE FAILURE CRITERION AND PROBABILISTIC FRACTURE ASSESSMENT CURVES FOR CERAMICSFatigue & Fracture of Engineering Materials & Structures, 1992
- Relation between shot-peening residual stress distribution and fatigue crack propagation life in spring steelTransactions of Japan Society of Spring Engineers, 1991
- FRACTURE AND DEFECT ASSESSMENT OF CERAMIC COMPOSITESFatigue & Fracture of Engineering Materials & Structures, 1990
- An empirical stress-intensity factor equation for the surface crackEngineering Fracture Mechanics, 1981
- Prediction of non propagating cracksEngineering Fracture Mechanics, 1979