Tribology of Different Ceramic Sliders on Lubricated Thin-Film Disks©
Authors:
- 1 January 1997
- journal article
- research article
- Published by Taylor & Francis in Tribology Transactions
- Vol. 40 (1) , 156-162
Abstract
Seventy-percent straight-rail, taper-flat sliders were made from A12O3-TiC, Mn-Zn ferrite, SiC, Si3N4 and ZrO2 and tested, on lubricated thin-film disks. The tests involved low speed (0.44 m/s) continuous contact drag testing at a fixed radius for a maximum of one. million revolutions or to disk failure. SiC did not cause the disk media, to fail, even, out to five million revolutions, and the friction force had. consistently low modulation throughout the test. Si3N4 did not cause any disk failures but exhibited higher friction force with more modulation. A2O3-TiC, Mn-Zn ferrite and ZrO2 exhibited high failure, rates (>50%), even though the initial friction forces were. low. The failure rates of these ceramics can be explained by the catalytic activity of Al2O3, TiC, Fe2O2 and ZrO2 on the degradation of the disk lubricant. Another explanation is the localized surface oxidation of SiC and Si3N4 sliders resulted, in a softer slider material exhibiting more wear, leading to higher contact area and lower contact stresses at the slider/disk interface.Keywords
This publication has 6 references indexed in Scilit:
- Degradation of Thin-Film Disk PFPE Lubricants by Ceramic Powders©Tribology Transactions, 1997
- Tribological Effects of Some Hydrocarbons on the Head/Disk InterfaceTribology Transactions, 1995
- Tribological and recording performance of carbon-coated thin film head sliders on unlubricated and lubricated thin film mediaIEEE Transactions on Magnetics, 1994
- Real contact area measurements on magnetic rigid disksWear, 1990
- Acidic Attack of Perfluorinated Alkyl Ether Lubricant Molecules by Metal Oxide SurfacesTribology Transactions, 1990
- Tribology and Mechanics of Magnetic Storage Devices1990