Effect of cooling rate and crack propagation direction on the mode 1 interlaminar fracture toughness of biaxial noncrimp warp‐knitted fabric composites made of glass/PP commingled yarn
Authors:
- 26 December 2007
- journal article
- research article
- Published by Wiley in Polymer Composites
- Vol. 29 (3) , 245-251
Abstract
The mode 1 interlaminar fracture toughness of biaxial (±45°) noncrimp warp‐knitted fabric composites made of glass/PP commingled yarn was investigated. The crack propagation along the warp and weft directions, respectively, was considered for the composites cooled at two different rates during laminate molding. The interlaminar fracture toughness was characterized by determining the critical strain energy release rate (GIC) of initiation and propagation measured from the double cantilever beam tests. In the case of a slow cooling rate (1°C/min), most specimens possess pure interlaminar crack propagation and direction‐independence characteristics. Nevertheless, the high‐cooled (10°C/min) specimens fractured in both directions suffer extensive intraply damage (crack branching, debonding, and bridging of 45°‐oriented interfacial yarns) and knit thread breakage, leading to GIC of propagation two times higher than that of the slow‐cooled specimens, and the clear difference in the GIC values of initiation between the two directions may be due to the contribution of the knit thread breakage to the fracture energy. POLYM. COMPOS., 2008 © 2007 Society of Plastics EngineersKeywords
This publication has 17 references indexed in Scilit:
- Mode I interlaminar fracture of woven glass/epoxy multidirectional laminatesComposites Part A: Applied Science and Manufacturing, 2005
- Mode I interlaminar fracture of carbon/epoxy multidirectional laminatesComposites Science and Technology, 2004
- Analysis of crack propagation in double cantilever beam tests of multidirectional laminatesMechanics of Materials, 2003
- Fracture toughness of weft-knitted fabric compositesComposites Part B: Engineering, 2002
- The effect of weave pattern on the mode-I interlaminar fracture energy of E-glass/vinyl ester compositesComposites Science and Technology, 2002
- Mode-I interlaminar fracture of carbon/epoxy cross-ply compositesComposites Science and Technology, 2002
- Fracture toughness evaluation for multidirectional CFRP by the Raman coating methodComposites Science and Technology, 2000
- Initiation and bifurcation mechanisms of cracks in multi-directional laminatesComposites Science and Technology, 2000
- The effect of weave pattern and crack propagation direction on mode I delamination resistance of woven glass and carbon compositesComposites Part B: Engineering, 1998
- A fractographic analysis of delamination within multidirectional carbon/epoxy laminatesComposites Science and Technology, 1995