Abstract
The effect of combined Cu and Ti additions on the magnetic properties and phase transformation behavior of Nd 8 Fe 86 B 6 nanocomposites prepared by melt spinning have been investigated. For pure ternary Nd 8 Fe 86 B 6 ribbons, the α–Fe phase precipitates directly from amorphous phase and its grains grow quickly during crystallization. But for Nd 8 Fe 86 B 6 ribbons with a combined addition of Cu and Ti, the crystallization temperature is increased by about 30 °C and a metastable hexagonal phase with a TbCu 7 -type structure is formed prior to the α–Fe and Nd 2 Fe 14 B phase. When the annealing temperature is increased, a metastable 1:7 phase is decomposed into the α–Fe and Nd 2 Fe 14 B phase. At the same time, the growth of α–Fe grains is suppressed and the microstructure becomes more uniform. When the content of Cu reaches 1.0 at. % and that of Ti reaches 0.5 at. %, the optimal magnetic properties i H c =4.8 kOe , σ r =110 emu/g , ( BH ) max =15 MGOe were obtained after annealing at the temperature of 650 °C for 8 min. So, a combined addition of Cu and Ti is very effective in improving the magnetic properties and reducing grain size and, in particular, the size of α–Fe grains.

This publication has 19 references indexed in Scilit: