Surface Exchange and Bulk Diffusivity of LSCF as SOFC Cathode: Electrical Conductivity Relaxation and Isotope Exchange Characterizations
Authors:
- 29 January 2013
- journal article
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 160 (4) , F343-F350
Abstract
The oxygen diffusion coefficient (D) and surface exchange coefficient (k) of a typical SOFC cathode material, La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) were characterized by both electrical conductivity relaxation (ECR) and oxygen isotope exchange (IE) methods. Conductivity relaxation experiments were conducted at 800°C for small step changes in partial pressure of oxygen ( PO2PO2 ), both decreasing and increasing, from 0.02 atm to 0.20 atm. The results revealed PO2PO2 dependent hysteresis with the reduction process requiring more equilibration time than oxidation. Analysis of the experimental data indicated that the surface exchange coefficient is a function of the final oxygen partial pressure in an isothermal system. In addition, both forward and backward oxygen reduction reaction constants, which are vital for the fundamental understanding of SOFC cathode reaction mechanisms, are investigated based on the relationship between surface exchange coefficient and PO2PO2 . The direct comparisons between the results from both ECR and IE were presented and the possible experimental errors in both methods were discussed.Keywords
This publication has 34 references indexed in Scilit:
- Determination of Surface Exchange Coefficients of LSM, LSCF, YSZ, GDC Constituent Materials in Composite SOFC CathodesJournal of the Electrochemical Society, 2011
- A novel pulse isotopic exchange technique for rapid determination of the oxygen surface exchange rate of oxide ion conductorsPhysical Chemistry Chemical Physics, 2009
- Defect chemistry and oxygen transport of (La0.6Sr0.4−xMx)0.99Co0.2Fe0.8O3−δ, M=Ca (x=0.05, 0.1), Ba (x=0.1, 0.2), SrPart I: Defect chemistrySolid State Ionics, 2009
- Investigating Oxygen Surface Exchange Kinetics of La[sub 0.8]Sr[sub .20]MnO[sub 3-δ] and La[sub 0.6]Sr[sub 0.4]Co[sub 0.2]Fe[sub 0.8]O[sub 3-δ] Using an Isotopic TracerJournal of the Electrochemical Society, 2008
- A novel application of mixed-valence Keggin-type polyoxometalates as non-aqueous electrolytes in polyacenic semiconductor secondary batteriesSolid State Ionics, 2003
- High temperature properties of La0.6Sr0.4Co0.8Fe0.2O3−δ oxygen nonstoichiometry and chemical diffusion constantSolid State Ionics, 2003
- Reactor Flush Time Correction in Relaxation ExperimentsJournal of the Electrochemical Society, 2001
- Chemical diffusivity of BaTiO3−Solid State Ionics, 1999
- Chemical diffusion and oxygen exchange of La0.6Sr0.4Co0.6Fe0.4O3−δSolid State Ionics, 1997
- A mathematical model of the porous SOFC cathodeSolid State Ionics, 1996