MICROSTRUCTURAL CHARACTERIZATION AND TENSILE PROPERTIES ASSESSMENT OF GTAW WELDED INCOLOY 800H ALLOYS FUEL CLADDING FOR SCWR
Authors:
- 1 January 2021
- journal article
- research article
- Published by Canadian Nuclear Laboratories Limited in CNL Nuclear Review
- Vol. 10 (1) , 20-29
Abstract
Incoloy 800H is one of several candidates for a fuel cladding material in super-critical water nuclear reactor concepts. The objective of this work is to determine the effect of the gas tungsten arc welding (GTAW) process on the microstructure and resulting tensile properties of Incoloy 800H tubes. In this work, GTAW was used to join Incoloy 800H. During welding, the weld thermal cycle produces differently featured heat-affected zone and fusion zone (FZ) microstructures. Microstructural examination revealed that weld-characteristic columnar and equiaxed dendritic structures were formed in the FZ. In comparison with the optimum heat input, both increase and decrease of heat input led to the formation of more columnar dendritic structures in the FZ. The chemical element distribution analysis using scanning electron microscopy/energy dispersive X-ray spectroscopy showed the segregation of Ti in the form of Ti-rich carbides and nitrides; other elements did not display any obvious segregation. Tensile test results revealed that Incoloy 800H alloy welds exhibit an excellent combination of strength and ductility almost equal to the base metal (BM) at the optimum and higher than optimum heat input conditions with full penetration. The welding process has no obvious effect on the microhardness across the whole welding zone. The refinement of grain size and morphology in the FZ can contribute to the improvement in the mechanical properties. As a result, the Incoloy 800H weldment shows the comparable mechanical properties to the BM.Keywords
This publication has 18 references indexed in Scilit:
- Microstructural Evolutions During Thermal Aging of Alloy 625: Impact of Temperature and Forming ProcessMetallurgical and Materials Transactions A, 2014
- Brazing Inconel 625 Using Two Ni/(Fe)-Based Amorphous Filler FoilsMetallurgical and Materials Transactions A, 2012
- Study on the Technology of Explosive Welding Incoloy800-SS304Journal of Materials Engineering and Performance, 2010
- Room temperature tensile behavior of service exposed and thermally aged service exposed alloy 625Scripta Materialia, 2001
- Microstructure and mechanical properties of Inconel 625 superalloyJournal of Nuclear Materials, 2001
- Microstructural features of dissimilar welds between 316LN austenitic stainless steel and alloy 800Materials Science and Engineering: A, 2000
- Precipitation of an intermetallic phase with Pt2Mo-type structure in alloy 625Metallurgical and Materials Transactions A, 1999
- Influence of heat treatments on microstructure, mechanical properties, and corrosion resistance of weld alloy 625Metallurgical and Materials Transactions A, 1995
- Effect of aging on the microstructure and tensile properties of an alloy 800/9Cr-1Mo steel jointInternational Journal of Pressure Vessels and Piping, 1995
- The performance of Alloy 625 in long-term intermediate temperature applicationsInternational Journal of Pressure Vessels and Piping, 1994