Abstract
Aqueous solutions of phosphotungstic acid were used to stain melt‐crystallized polypropylene which had been oxidized to the leveled‐off stage by boiling in 70% HNO3. Electron microscopy of thin sections of the polymer revealed unstained crystalline lamellae bordered by stained interlamellar layers. The lamella height, which is equivalent to the fold period of the molecules, increased as the crystallization temperature increased. In polypropylene which had crystallized in ice water, and at 125, 145, or 161°C., the heights of the visually delineated lamellae were 80, 105, 158, and 210 A., respectively. Those heights were, in turn, approximately the same as the length of the perpendicularly aligned molecules in the lamellae, which survived the acid etch. The stained interlamellar layers, regardless of the crystallization temperature, were about half the height of the lamellae.

This publication has 3 references indexed in Scilit: