Interfacial Interactions and Flammability of Flame-Retarded and Short Fiber-Reinforced Polyamides
- 8 September 2009
- journal article
- research article
- Published by Taylor & Francis in Polymer-Plastics Technology and Engineering
- Vol. 48 (10) , 1046-1054
Abstract
Interfacial properties, crystallinity and flammability of short fiber reinforced and flame retarded polyamide 6 and polyamide 66 compounds are investigated, emphasizing the influence of flame retardant fillers on the resistance of fiber/matrix interface to shear. Interfacial shear strengths are derived through a micromechanical approach by determining the tensile properties and residual fiber length distributions. Validated by fracture morphologies, interfacial strengths are found to be governed by filler – induced apparent crystallinities and fractional occurrence of polyamide polymorphs, obtained via peak deconvolution of X-Ray diffraction patterns. Although flame retardant additives based on Br/Sb synergism are found to impart excellent flammability reductions regarding oxygen index and UL94 classifications (V-0 rating), degree of crystallinity; thus, interfacial properties are deteriorated due to lowered thermal expansion and increased cooling rates. Red phosphorus as a flame retardant also induces a UL94 V-0 and significant reduction in flammability together with the facts that crystallinity is not altered and a strong fiber/matrix interface is maintained. Use of melamine cyanurate in an unreinforced polyamide improves the limiting oxygen index considerably; however, the UL94 rating remains unchanged as V-2 as a consequence of increased level of melt dripping. Melamine cyanurate additionally increases the degree of crystallinity through promotion of heterogeneous nucleation.Keywords
This publication has 31 references indexed in Scilit:
- Polyamide 6 Filled with Melamine Cyanurate and Layered Silicates: Evaluation of Flame Retardancy and Physical PropertiesMacromolecular Materials and Engineering, 2008
- Strength of short fiber reinforced polymers: Effect of fiber length distributionPolymer Composites, 2008
- Thermal Stability and Properties of Flame Retarded Glass Fiber Reinforced Polyamide 66 CompositeJournal of Reinforced Plastics and Composites, 2007
- Preparation of polyamide resin‐encapsulated melamine cyanurate/melamine phosphate composite flame retardants and the fire‐resistance to glass fiber‐reinforced polyamide 6Journal of Applied Polymer Science, 2006
- Hydrogen bonding, mobility, and structural transitions in aliphatic polyamidesJournal of Polymer Science Part B: Polymer Physics, 2006
- Preparation and Combustion Properties of Flame Retardant Nylon 6/Montmorillonite NanocompositeMacromolecular Materials and Engineering, 2003
- Effect of melamine polyphosphate on thermal degradation of polyamides: a combined X-ray diffraction and solid-state NMR studyPolymer, 2003
- Effects of fiber length and fiber orientation distributions on the tensile strength of short-fiber-reinforced polymersComposites Science and Technology, 1996
- On the re-inforcement of thermoplastics by imperfectly aligned discontinuous fibresJournal of Materials Science, 1972
- Tensile properties of fibre-reinforced metals: Copper/tungsten and copper/molybdenumJournal of the Mechanics and Physics of Solids, 1965